Abstract: The invention relates to a method and equipment of producing with good reproducibility steel which is extremely free from slag inclusions, particularly steel with low sulphur content and thus very low contents of sulphidic slag inclusions, starting with a steel melt which is decarburized in a melting furnace, converter or the like to the desired carbon content, after which subsequent refining is carried out by an injection method in a ladle.