Abstract: The present invention relates to a manufacturing method of a porous ceramic material, which includes the following steps: mixing a silicate material and a porogen to obtain a premix, wherein the silicate material includes sodium silicate and other compounds being at least one selected from the group consisting of oxides, nitrides, and carbides; drying the premix to obtain a silicate aggregate; mixing the silicate aggregate and an adhesive to obtain an injection molding material, wherein in a weight percentage, the silicate aggregate is in the range of from 50% to 60%, the adhesive is in the range of from 40% to 50%; injection molding the injection molding material to obtain a green body; and degumming and calcinating the green body successively to obtain the porous ceramic material.