Abstract: The invention relates to methods for producing cesium hydroxide solutions during which: cesium-containing ore is disintegrated with sulfuric acid while forming a cesium aluminum sulfate hydrate, which is poorly soluble at low temperatures; the formed cesium alum is separated away in the form of a solution from the solid ore residues; the aluminum is precipitated out of the cesium alum solution while forming a cesium sulfate solution; the formed cesium sulfate solution is reacted with barium hydroxide or stontium hydroxide while forming a cesium hydroxide solution, and; the formed cesium hydroxide solution is concentrated and purified.