Abstract: Ceramic structure having porosity of 10-80% is characterized by a solid cmic matrix having therein elongated and parallel channels, the structure is made by a process that includes the steps of:(a) arranging tows of elongated fibers parallel to each other to form a fiber preform,(b) contacting the fiber preform with a matrix precursor whereby the matrix precursor deposits around the fibers,(c) removing the fiber preform from the matrix precursor,(d) drying the fiber preform,(e) calcining the fiber preform,(f) hot pressing the structure containing the fugitive fibers therein, and(g) removing at least some of the fibers to form channels in the structure.
Type:
Grant
Filed:
December 20, 1996
Date of Patent:
January 12, 1999
Assignee:
Tht United States of America as represented by the Secretary of the Navy