Abstract: A process for coating a steel strip, particularly ferritic stainless steel, with aluminum by hot quenching, in which the strip is preheated to a temperature less than 500.degree. C. in a first non-oxidizing atmosphere containing a quantity of oxygen less than 3%, the strip is then heated to a temperature less than 950.degree. C. in a second non-oxidizing atmosphere, the strip is then conveyed to an atmosphere (3, 4) which is non-reactive at the coating temperature, and, finally, the strip is quenched in a coating bath.
Type:
Grant
Filed:
April 5, 1993
Date of Patent:
October 25, 1994
Assignees:
Sollac, Ugine, Aciers de Chatillon & Gueugnon
Inventors:
Eric Buscarlet, Charles G. Brun, Danielle Quantin, Jean-Paul Hennechart, Marc Mantel, Patrice de Veyrac, Bernard Baroux