Patents Assigned to WISHBONE
-
Patent number: 12779087Abstract: The present invention relates to a bone regeneration material comprising: a solid first phase of hydroxyapatite of natural origin which is macroporous, having pores of diameters greater than or equal to 50 ?m, this phase of hydroxyapatite is a crystalline solid phase of hydroxyapatite, whose crystals have a size comprised between 20 and 120 nm, and this solid phase of hydroxyapatite has a specific surface area comprised between 8 and 20 m2/g, the method of production and a method of bone repair based on this bone regeneration material.Type: GrantFiled: December 23, 2021Date of Patent: November 3, 2026Assignee: WishboneInventors: Eric Rompen, Geoffrey Lecloux, France Lambert, Emilie Dory
-
Publication number: 20250352698Abstract: A bone regeneration material containing a solid first phase of hydroxyapatite of natural origin which is macroporous, having pores of diameters greater than or equal to 50 pm, and a solid synthetic second phase of calcium phosphate intended to enrich the first phase and having a Ca/P molar ratio of between 0.2 and 2 is provided. The bone regeneration material has a defined weight ratio of the solid first phase of hydroxyapatite of natural origin to the solid synthetic second phase of calcium phosphate of between 99/1 and 1/99.Type: ApplicationFiled: August 1, 2025Publication date: November 20, 2025Applicant: WishboneInventors: Emilie DORY, Eric ROMPEN, France LAMBERT, Geoffrey LECLOUX
-
Publication number: 20220111117Abstract: The present invention relates to a bone regeneration material comprising: a solid first phase of hydroxyapatite of natural origin which is macroporous, having pores of diameters greater than or equal to 50 ?m, this phase of hydroxyapatite is a crystalline solid phase of hydroxyapatite, whose crystals have a size comprised between 20 and 120 nm, and this solid phase of hydroxyapatite has a specific surface area comprised between 8 and 20 m2/g, the method of production and a method of bone repair based on this bone regeneration material.Type: ApplicationFiled: December 23, 2021Publication date: April 14, 2022Applicant: WishboneInventors: Eric ROMPEN, Geoffrey LECLOUX, France LAMBERT, Emilie DORY
-
Publication number: 20200121827Abstract: The present invention relates to a bone regeneration material comprising: a solid first phase of hydroxyapatite of natural origin which is macroporous, having pores of diameters greater than or equal to 50 pm, preferably pores of diameters between 50 and 100 pm, and a solid synthetic second phase of calcium phosphate intended to enrich said first phase, said second phase having a Ca/P molar ratio of between 0.2 and 2, preferably of between 0.3 and 1.9, preferentially of between 0.5 and 1.65, said bone regeneration material having a defined weight ratio of said solid first phase of hydroxyapatite of natural origin to said solid synthetic second phase of calcium phosphate of between 99/1 and 1/99.Type: ApplicationFiled: January 15, 2018Publication date: April 23, 2020Applicant: WishboneInventors: Emilie DORY, Eric ROMPEN, France LAMBERT, Geoffrey LECLOUX
-
Patent number: 10251974Abstract: Described herein is a method that comprises: —placing a bone material, containing hydroxyapatite and organic substances, in contact with an extraction liquid that gives rise to a first liquid phase, containing the organic substances and possibly impurities extracted from the bone material, and a second solid hydroxyapatite phase, containing the hydroxyapatite; and —separating the liquid phase and the solid hydroxyapatite phase. The extraction liquid is an aqueous extraction solution brought to a temperature between 150° C. and 300° C. and a pressure between 150 kPa and 350 kPa.Type: GrantFiled: October 2, 2014Date of Patent: April 9, 2019Assignee: WishboneInventors: Eric Rompen, France Lambert, Geoffrey Lecloux, Philippe Moniotte
-
Publication number: 20160235885Abstract: The invention relates to a method that includes: placing a bone material, containing hydroxyapatite and organic substances, in contact with an extraction liquid that gives rise to a first liquid phase, containing said organic substances and possibly impurities extracted from said bone material, and a second solid hydroxyapatite phase, containing said hydroxyapatite; and separating said liquid phase and said solid hydroxyapatite phase. Said extraction liquid is an aqueous extraction solution brought to a temperature between 150° C. and 300° C. and a pressure between 150 kPa and 350 kPa.Type: ApplicationFiled: October 2, 2014Publication date: August 18, 2016Applicant: WISHBONEInventors: Eric Rompen, France Lambert, Geoffrey Lecloux, Philippe Moniotte