Abstract: A thermoelectric material and a method of making a thermoelectric material are provided. In certain embodiments, the thermoelectric material comprises at least 10 volume percent porosity. In some embodiments, the thermoelectric material has a zT greater than about 1.2 at a temperature of about 375 K. In some embodiments, the thermoelectric material comprises a topological thermoelectric material. In some embodiments, the thermoelectric material comprises a general composition of (Bi1-xSbx)u(Te1-ySey)w, wherein 0?x?1, 0?y?1, 1.8?u?2.2, 2.8?w?3.2. In further embodiments, the thermoelectric material includes a compound having at least one group IV element and at least one group VI element. In certain embodiments, the method includes providing a powder comprising a thermoelectric composition, pressing the powder, and sintering the powder to form the thermoelectric material.
Type:
Grant
Filed:
March 30, 2012
Date of Patent:
August 5, 2014
Assignees:
ZT Plus, The Ohio State University
Inventors:
Joseph P. Heremans, Christopher M. Jaworski, Vladimir Jovovic, Fred Harris
Abstract: A thermoelectric material and a method of forming a thermoelectric material are provided. The method of forming a thermoelectric material includes providing at least one compound fabricated by a first technique and having a first power factor and a first thermal conductivity. The method further includes modifying a spatial structure of the at least one compound by a second technique different from the first technique. The modified at least one compound has a plurality of portions separated from one another by a plurality of boundaries. The plurality of portions include one or more portions having a second power factor not less than the first power factor, and the modified at least one compound has a second thermal conductivity less than the first thermal conductivity.
Abstract: A thermoelectric material and a method of making a thermoelectric material are provided. In certain embodiments, the thermoelectric material comprises at least 10 volume percent porosity. In some embodiments, the thermoelectric material has a zT greater than about 1.2 at a temperature of about 375 K. In some embodiments, the thermoelectric material comprises a topological thermoelectric material. In some embodiments, the thermoelectric material comprises a general composition of (Bi1-xSbx)u(Te1-ySey)w, wherein 0?x?1, 0?y?1, 1.8?u?2.2, 2.8?w?3.2. In further embodiments, the thermoelectric material includes a compound having at least one group IV element and at least one group VI element. In certain embodiments, the method includes providing a powder comprising a thermoelectric composition, pressing the powder, and sintering the powder to form the thermoelectric material.
Type:
Application
Filed:
March 30, 2012
Publication date:
October 4, 2012
Applicants:
THE OHIO STATE UNIVERSITY, ZT PLUS
Inventors:
Joseph P. Heremans, Christopher M. Jaworski, Vladimir Jovovic, Fred Harris
Abstract: Improved thermoelectric assemblies are disclosed, wherein layers of heterostructure thermoelectric materials or thin layers of thermoelectric material form thermoelectric elements. The layers are bound together with agents that improve structural strengths, allow electrical current to pass in a preferred direction, and minimize or reduce adverse affects, such a shear stresses, that might occur to the thermoelectric properties and materials of the assembly by their inclusion.
Abstract: Improved thermoelectric assemblies are disclosed, wherein layers of heterostructure thermoelectric materials or thin layers of thermoelectric material form thermoelectric elements. The layers are bound together with agents that improve structural strengths, allow electrical current to pass in a preferred direction, and minimize or reduce adverse affects, such a shear stresses, that might occur to the thermoelectric properties and materials of the assembly by their inclusion.