Abstract: A vitreous material suitable for coating a semiconductor component comprises, by weight:30% to 40% zinc oxide ZnO,15% to 30% lead oxide PbO,20% to 40% boron oxide B.sub.2 O.sub.3,5% to 20% silicon dioxide SiO.sub.2,2% to 10% aluminum titanate Al.sub.2 TiO.sub.5, and0% to 5% bismuth oxide Bi.sub.2 O.sub.3.
Type:
Grant
Filed:
July 9, 1982
Date of Patent:
October 11, 1983
Assignee:
Societe Anonyme dite Compagnie General d'Electricite