Abstract: A method for producing polysuccinimide is provided. Thermal polymerization of maleamic acid at a temperature of from about 160.degree. C. to about 330.degree. C. produces polysuccinimide. The reaction is optionally conducted in the presence of one or more processing aids, solvents or diluents. The polysuccinimide is particularly useful as a detergent additive.
Type:
Grant
Filed:
October 13, 1992
Date of Patent:
February 28, 1995
Assignee:
Rohm and Haas Company
Inventors:
Michael B. Freeman, Yi H. Paik, Ethan S. Simon, Graham Swift