  • Patent number: 7592393
    Abstract: A polyolefin composition comprising: (A) from 8 to 25% by weight of a crystalline homopolymer or copolymer of propylene: (B) from 75 to 92% by weight of an elastomeric fraction comprising: (1) a first elastomeric copolymer of propylene with from 15 to 32% by weight at least one alpha-olefin of formula H2C?CHR, where R is H or a C2-6 linear or branched alkyl, optionally containing 0.5 to 5% by weight of a diene, said first elastomeric copolymer containing alpha-olefin, and having solubility in xylene at room temperature greater than 50% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from 3.0 to 5.0 dl/g; and (2) a second elastomeric copolymer of propylene with at least one alpha-olefin of formula H2C?CHR, where R is H or a C2-6 linear or branched alkyl, optionally containing 0.
    Type: Grant
    Filed: April 8, 2002
    Date of Patent: September 22, 2009
    Assignee: Basel Poliolefine Italia S.p.A.
    Inventors: Anteo Pelliconi, Enea Garagnani, Alvaro Villanueva
  • Publication number: 20050035520
    Abstract: This invention relates to an apparatus and method for making booklets. Such structures of this type, generally, employ a variety of creasing techniques in order to form the booklet.
    Type: Application
    Filed: September 24, 2004
    Publication date: February 17, 2005
    Inventors: Jose Alvaro Villanueva, Robert Lawton
  • Publication number: 20040198919
    Abstract: A polyolefin composition comprising: (A) from 8 to 25% by weight of a crystalline homopolymer or copolymer of propylene: (B) from 75 to 92% by weight of an elastomeric fraction comprising: (1) a first elastomeric copolymer of propylene with from 15 to 32% by weight at least one alpha-olefin of formula H2C═CHR, where R is H or a C2-6 linear or branched alkyl, optionally containing 0.5 to 5% by weight of a diene, said first elastomeric copolymer containing alpha-olefin, and having solubility in xylene at room temperature greater than 50% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from 3.0 to 5.0 dl/g; and (2) a second elastomeric copolymer of propylene with at least one alpha-olefin of formula H2C═CHR, where R is H or a C2-6 linear or branched alkyl, optionally containing 0.