Patents by Inventor Andrea Kaeufler

Andrea Kaeufler has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9702027
    Abstract: The invention relates to a copper alloy, composed of (in wt %): 51.8 to 84.0% Cu, 15.5 to 36.0% Zn, 0.35 to 3.0% Sn, 0.12 to 1.5% Fe, 0.02 to 1.0% P, optionally also 0.1 to 2.0% Al, optionally also 0.05 to 0.7% Si, optionally also 0.05 to 2.0% Ni, optionally also respectively 0.1 to 1.0% Mn, Co, optionally also respectively 0.01 to 1.0% As, Sb, and unavoidable contaminants, wherein more than 95% of the structure consist of ?-mixed crystal, in which at least iron phosphides and/or iron are embedded as deposition particles, which can be used for metallic articles in breeding organisms living in seawater.
    Type: Grant
    Filed: June 15, 2012
    Date of Patent: July 11, 2017
    Assignee: WIELAND-WERKE AG
    Inventors: Andrea Kaeufler, Jochen Aufrecht
  • Patent number: 9493858
    Abstract: A copper alloy subjected to a thermo-mechanical treatment and composed of (in wt %) 15.5 to 36.0% Zn, 0.3 to 3.0% Sn, 0.1 to 1.5% Fe, optionally 0.001 to 0.4% P, optionally 0.01 to 0.1% Al, optionally 0.01 to 0.03% Ag, Mg, Zr, In, Co, Cr, Ti, Mn, optionally 0.05 to 0.5% Ni, the remainder being copper and unavoidable contaminants, wherein the microstructure of the alloy is characterized in that the proportions of the main texture orientations are at least 10 vl % copper orientation, at least 10 vl % S/R orientation, at least 5 vl % brass orientation, at least 2 vl % Goss orientation, at least 2 vl % 22RD-cube orientation, at least 0.5 vl % cube orientation, and finely distributed iron-containing particles are contained in the alloy matrix.
    Type: Grant
    Filed: June 15, 2012
    Date of Patent: November 15, 2016
    Assignee: WIELAND-WERKE AG
    Inventors: Hans-Achim Kuhn, Andrea Kaeufler, Stefan Gross
  • Publication number: 20140377127
    Abstract: The invention relates to a copper alloy that has been subjected to a thermo-mechanical treatment, composed of (in wt %) 15.5 to 36.0% Zn, 0.3 to 3.0% Sn, 0.1 to 1.5% Fe, optionally also 0.001 to 0.4% P, optionally also 0.01 to 0.1% Al, optionally also 0.01 to 0.03% Ag, Mg, Zr, In, Co, Cr, Ti, Mn, optionally also 0.05 to 0.5% Ni, the remainder copper and unavoidable contaminants, wherein the microstructure of the alloy is characterized in that the proportions of the main texture layers are at least 10 vl % copper layer, at least 10 vl % S/R layer, at least 5 vl % brass layer, at least 2 vl % Goss layer, at least 2 vl % 22RD-cube layer, at least 0.5 vl % cube layer, and finely distributed iron-containing particles are contained in the alloy matrix.
    Type: Application
    Filed: June 15, 2012
    Publication date: December 25, 2014
    Inventors: Hans-Achim Kuhn, Andrea Kaeufler, Stefan Gross
  • Publication number: 20140170016
    Abstract: The invention relates to the use of a copper alloy, composed of (in wt %): 51.8 to 84.0% Cu, 15.5 to 36.0% Zn, 0.35 to 3.0% Sn, 0.12 to 1.5% Fe, 0.02 to 1.0% P, optionally also 0.1 to 2.0% Al, optionally also 0.05 to 0.7% Si, optionally also 0.05 to 2.0% Ni, optionally also respectively 0.1 to 1.0% Mn, Co, optionally also respectively 0.01 to 1.0% As, Sb, and unavoidable contaminants, wherein more than 95% of the structure consist of ?-mixed crystal, in which at least iron phosphides and/or iron are embedded as deposition particles, for metallic articles in breeding organisms living in seawater.
    Type: Application
    Filed: June 15, 2012
    Publication date: June 19, 2014
    Inventors: Andrea Kaeufler, Jochen Aufrecht
  • Publication number: 20140161661
    Abstract: The invention relates to a copper alloy that has been subjected to a thermo-mechanical treatment, composed of (in wt %) 15.5 to 36.0% Zn, 0.3 to 3.0% Sn, 0.1 to 1.5% Fe, optionally also 0.001 to 0.4% P, optionally also 0.01 to 0.1% Al, optionally also 0.01 to 0.03% Ag, Mg, Zr, In, Co, Cr, Ti, Mn, optionally also 0.05 to 0.5% Ni, the remainder copper and unavoidable contaminants, wherein the microstructure of the alloy is characterized in that the proportions of the main texture layers are at least 10 vl % copper layer, at least 10 vl % S/R layer, at least 5 vl % brass layer, at least 2 vl % Goss layer, at least 2 vl % 22RD-cube layer, at least 0.5 vl % cube layer, and finely distributed iron-containing particles are contained in the alloy matrix.
    Type: Application
    Filed: June 15, 2012
    Publication date: June 12, 2014
    Inventors: Hans-Achim Kuhn, Andrea Kaeufler, Stefan Gross