  • Patent number: 7462255
    Abstract: Method for producing by laser gastight and high-temperature resistant connections of shaped parts made of non-oxidic ceramic. The invention relates to the fields of ceramics and laser technology and relates to a method with which, e.g., low-melting-point or radioactive materials can be enclosed inside a container made of ceramic. The object of the invention is to produce a durable, gastight and high-temperature resistant connection between components made of non-oxidic ceramic. Shaped parts made of the ceramic are provided on the surfaces to be joined with a solder of 80-30% by weight yttrium oxide and/or 55-15% by weight zirconium oxide, 20-70% by weight aluminum oxide, 0-50% by weight silicon dioxide and 0-10% by weight silicon, and subsequently the temperature at the joint area is increased above the melting temperature of the solder by means of a laser without the presence of a protective gas atmosphere or a vacuum.
    Type: Grant
    Filed: December 13, 2004
    Date of Patent: December 9, 2008
    Assignees: Technische Universitaet Dresden, Management Associates
    Inventors: Juergen Knorr, Wolfgang Lippmann, Regine Wolf, Horst Exner, Anne-Maria Reinecke
  • Publication number: 20050167409
    Abstract: Method for producing by laser gastight and high-temperature resistant connections of shaped parts made of non-oxidic ceramic. The invention relates to the fields of ceramics and laser technology and relates to a method with which, e.g., low-melting-point or radioactive materials can be enclosed inside a container made of ceramic. The object of the invention is to produce a durable, gastight and high-temperature resistant connection between components made of non-oxidic ceramic. Shaped parts made of the ceramic are provided on the surfaces to be joined with a solder of 80-30% by weight yttrium oxide and/or 55-15% by weight zirconium oxide, 20-70% by weight aluminum oxide, 0-50% by weight silicon dioxide and 0-10% by weight silicon, and subsequently the temperature at the joint area is increased above the melting temperature of the solder by means of a laser without the presence of a protective gas atmosphere or a vacuum.
    Type: Application
    Filed: December 13, 2004
    Publication date: August 4, 2005
    Applicants: TECHNISCHE UNIVERSITAET DRESDEN, HORST EXNER, ANNE-MARIA REINECKE
    Inventors: Juergen Knorr, Wolfgang Lippmann, Regine Wolf, Horst Exner, Anne-Maria Reinecke