  • Patent number: 8217117
    Abstract: An optical film having at least one layer formed of a polyolefin based resin composition containing 8 to 30 wt % of a component (A) defined below and 92 to 70 wt % of a component (B) defined below, with the proviso that the total of the component (A) and the component (B) is 100 wt %: component (A): an olefin based polymer with which neither a crystal fusion peak having a crystal fusion heat of 30 J/g or more nor a crystallization peak having a crystallization heat of 30 J/g or more to be observed in the range of ?50 to 200° C. is observed in a differential scanning calorimetry measurement according to JIS K 7122; and component (B): a propylene based polymer with which a crystal fusion peak having a crystal fusion heat larger than 30 J/g or a crystallization peak having a crystallization heat larger than 30 J/g to be observed in the range of ?50 to 200° C. is observed in a differential scanning calorimetry measurement according to JIS K 7122.
    Type: Grant
    Filed: September 18, 2008
    Date of Patent: July 10, 2012
    Assignee: Sumitomo Chemical Company, Limited
    Inventors: Kyoko Hino, Hiroaki Takahata, Ayako Yada
  • Publication number: 20100222517
    Abstract: An optical film having at least one layer formed of a polyolefin based resin composition containing 8 to 30 wt % of a component (A) defined below and 92 to 70 wt % of a component (B) defined below, with the proviso that the total of the component (A) and the component (B) is 100 wt %: component (A): an olefin based polymer with which neither a crystal fusion peak having a crystal fusion heat of 30 J/g or more nor a crystallization peak having a crystallization heat of 30 J/g or more to be observed in the range of ?50 to 200° C. is observed in a differential scanning calorimetry measurement according to JIS K 7122; and component (B): a propylene based polymer with which a crystal fusion peak having a crystal fusion heat larger than 30 J/g or a crystallization peak having a crystallization heat larger than 30 J/g to be observed in the range of ?50 to 200° C. is observed in a differential scanning calorimetry measurement according to JIS K 7122.
    Type: Application
    Filed: September 18, 2008
    Publication date: September 2, 2010
    Applicant: Sumitomo Chemical Company, Limited
    Inventors: Kyoko Hino, Hiroaki Takahata, Ayako Yada
  • Publication number: 20040158000
    Abstract: There is provided a polypropylene resin composition comprising the following components (A) and (B):
    Type: Application
    Filed: September 15, 2003
    Publication date: August 12, 2004
    Applicant: SUMITOMO CHEMICAL COMPANY, LIMITED
    Inventors: Ayako Yada, Hiroyuki Tanimura