  • Patent number: 9212234
    Abstract: In a process for producing high molecular weight polyethylene, ethylene is contacted with a slurry of a catalyst composition comprising a Group 4 metal complex of a phenolate ether ligand under polymerization conditions comprising a temperature of about 20° C. to less than 90° C. and a pressure of about 4 bar to about 40 bar.
    Type: Grant
    Filed: July 1, 2011
    Date of Patent: December 15, 2015
    Assignee: TICONA GMBH
    Inventors: Dominique Robert, Julia Hufen, Kerstin Lüdtke, Bjorn Rinker, Jens Ehlers
  • Publication number: 20140004339
    Abstract: A polyethylene powder is described having a molecular weight in the range of from 3,000,000 g/mol to less than 4,000,000 g/mol as determined by ASTM 4020 and a bulk density of 0.10 to 0.20 g/cm3. On sintering, the polyethylene powder produces a porous article having an elastic modulus of at least 90 MPa.
    Type: Application
    Filed: April 6, 2012
    Publication date: January 2, 2014
    Inventors: Jens Ehlers, Kerstin Lüdtke, Julia Hufen, Ramesh Srinivasan, Björn Rinker
  • Publication number: 20130072649
    Abstract: In a process for producing high molecular weight polyethylene, ethylene is contacted with a slurry of a catalyst composition comprising a Group 4 metal complex of a phenolate ether ligand under polymerization conditions comprising a temperature of about 20° C. to less than 90° C. and a pressure of about 4 bar to about 40 bar.
    Type: Application
    Filed: July 1, 2011
    Publication date: March 21, 2013
    Applicant: TICONA GMBH
    Inventors: Dominique Robert, Julia Hufen, Kerstin Lüdtke, Bjorn Rinker, Jens Ehlers
  • Publication number: 20130046040
    Abstract: A polyethylene powder has a molecular weight in the range of about 300,000 g/mol to about 2,000,000 g/mol as determined by ASTM-D 4020, an average particle size, D50, between about 300 and about 1500 ?m, and a bulk density between about 0.25 and about 0.5 g/ml. On sintering, the polyethylene powder produces a porous article having a porosity of at least 45% and a pressure drop less than 5 mbar. The porous article is useful in, for example, wastewater aeration and capillary and filtration applications.
    Type: Application
    Filed: May 3, 2011
    Publication date: February 21, 2013
    Applicant: TICONA LLC