  • Patent number: 8569200
    Abstract: A catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Grant
    Filed: December 1, 2011
    Date of Patent: October 29, 2013
    Assignee: LG Chem, Ltd.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Patent number: 8492305
    Abstract: The present invention relates to a catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Grant
    Filed: December 1, 2011
    Date of Patent: July 23, 2013
    Assignee: LG Chem, Ltd.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Patent number: 8242047
    Abstract: The present invention relates to an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking, method for preparing the same and a method for preparing olefin by using the same. More precisely, the present invention relates to an oxide catalyst for hydrocarbon steam cracking represented by formula 1 and a phosphoric oxide catalyst for hydrocarbon steam cracking represented by formula 3 which would be used for the production of olefin such as ethylene and propylene by hydrocarbon steam cracking, and a method for preparing the same. The present invention provides an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking that has excellent thermo-stability at high temperature and improved olefin yield. CrZrjAkOx??[Formula 1] CrZrjAkPlOx??[Formula 3] Wherein, j, k, l and x are as indicated in the description.
    Type: Grant
    Filed: March 25, 2011
    Date of Patent: August 14, 2012
    Assignee: LG Chem, Ltd.
    Inventors: Jun-seon Choi, Jun-Han Kang, Jong-hun Song, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Publication number: 20120108417
    Abstract: The present invention relates to a catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Application
    Filed: December 1, 2011
    Publication date: May 3, 2012
    Applicant: LG CHEM, LTD.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Publication number: 20120108416
    Abstract: A catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Application
    Filed: December 1, 2011
    Publication date: May 3, 2012
    Applicant: LG CHEM, LTD.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Patent number: 8123931
    Abstract: The present invention relates to a catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Grant
    Filed: May 23, 2008
    Date of Patent: February 28, 2012
    Assignee: LG Chem, Ltd.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Publication number: 20110172483
    Abstract: The present invention relates to an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking, method for preparing the same and a method for preparing olefin by using the same. More precisely, the present invention relates to an oxide catalyst for hydrocarbon steam cracking represented by formula 1 and a phosphoric oxide catalyst for hydrocarbon steam cracking represented by formula 3 which would be used for the production of olefin such as ethylene and propylene by hydrocarbon steam cracking, and a method for preparing the same. The present invention provides an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking that has excellent thermo-stability at high temperature and improved olefin yield. CrZrjAkOx ??[Formula 1] CrZrjAkPlOx ??[Formula 3] Wherein, j, k, l and x are as indicated in the description.
    Type: Application
    Filed: March 25, 2011
    Publication date: July 14, 2011
    Inventors: Jun-seon CHOI, Jun-Han Kang, Jong-hun Song, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Patent number: 7951987
    Abstract: The present invention relates to a thermal-cracking method of hydrocarbon using a hydrocarbon thermal-cracking apparatus including a tube type furnace having a radiation part for thermally cracking hydrocarbon feedstocks supplied together with steam and a convection part. A hydrocarbon thermal-cracking catalyst is packed in some or entire area of the tube placed in the radiation part of the tube type furnace, wherein the hydrocarbon thermal-cracking catalyst includes an oxide catalyst represented by CrZrjAkOx (wherein, 0.5?j?120 and 0?k?50, A is a transition metal, and x is a number corresponding to the atomic values of Cr, Zr, and A and the numbers of j and k). Therefore, it is possible to improve yield and selectivity of olefin, reduce fuel consumption due to an excellent heat transfer efficiency and extend decoking interval by reduced production of coke deposited to an inside wall of a tube, in steam cracking of hydrocarbon for producing olefin.
    Type: Grant
    Filed: July 2, 2008
    Date of Patent: May 31, 2011
    Assignee: LG Chem, Ltd.
    Inventors: Jun-seon Choi, Byoung-gi Park, Jin-do Kim, Hyune-jung Ryu
  • Patent number: 7935654
    Abstract: The present invention relates to an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking, method for preparing the same and a method for preparing olefin by using the same. More precisely, the present invention relates to an oxide catalyst for hydrocarbon steam cracking represented by formula 1 and a phosphoric oxide catalyst for hydrocarbon steam cracking represented by formula 3 which would be used for the production of olefin such as ethylene and propylene by hydrocarbon steam cracking, and a method for preparing the same. The present invention provides an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking that has excellent thermo-stability at high temperature and improved olefin yield. CrZrjAkOx??[Formula 1] CrZrjAkPlOx??[Formula 3] Wherein, j, k, l and x are as indicated in the description.
    Type: Grant
    Filed: September 24, 2007
    Date of Patent: May 3, 2011
    Assignee: LG Chem, Ltd.
    Inventors: Jun-seon Choi, Jun-Han Kang, Jong-hun Song, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Patent number: 7897122
    Abstract: A hybrid adsorbent-membrane reactor in which the chemical reaction, membrane separation, and product adsorption are coupled. Also disclosed are a dual-reactor apparatus and a process using the reactor or the apparatus.
    Type: Grant
    Filed: February 14, 2006
    Date of Patent: March 1, 2011
    Assignees: Media and Process Technology, LG Petrochemical Co., Ltd., University of Southern California
    Inventors: Theodore T. Tsotsis, Muhammad Sahimi, Babak Fayyaz-Najafi, Aadesh Harale, Byoung-Gi Park, Paul K. T. Liu
  • Publication number: 20090105066
    Abstract: The present invention relates to a catalyst for hydrocarbon steam cracking for the production of light olefin, a preparation method of the catalyst and a preparation method of olefin by using the same. More precisely, the present invention relates to a composite catalyst prepared by mixing the oxide catalyst powder represented by CrZrjAkOx (0.5?j?120, 0?k?50, A is a transition metal, x is the number satisfying the condition according to valences of Cr, Zr and A, and values of j and k) and carrier powder and sintering thereof, a composite catalyst wherein the oxide catalyst is impregnated on a carrier, and a method of preparing light olefin such as ethylene and propylene by hydrocarbon steam cracking in the presence of the composite catalyst. The composite catalyst of the present invention has excellent thermal/mechanical stability in the cracking process, and has less inactivation rate by coke and significantly increases light olefin yield.
    Type: Application
    Filed: May 23, 2008
    Publication date: April 23, 2009
    Applicant: LG Chem, Ltd.
    Inventors: Jun-han Kang, Jong-hun Song, Jun-seon Choi, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Publication number: 20090012340
    Abstract: The present invention relates to a thermal-cracking method of hydrocarbon using a hydrocarbon thermal-cracking apparatus including a tube type furnace having a radiation part for thermally cracking hydrocarbon feedstocks supplied together with steam and a convection part. A hydrocarbon thermal-cracking catalyst is packed in some or entire area of the tube placed in the radiation part of the tube type furnace, wherein the hydrocarbon thermal-cracking catalyst includes an oxide catalyst represented by CrZrjAkOx (wherein, 0.5?j?120 and 0?k?50, A is a transition metal, and x is a number corresponding to the atomic values of Cr, Zr, and A and the numbers of j and k). Therefore, it is possible to improve yield and selectivity of olefin, reduce fuel consumption due to an excellent heat transfer efficiency and extend decoking interval by reduced production of coke deposited to an inside wall of a tube, in steam cracking of hydrocarbon for producing olefin.
    Type: Application
    Filed: July 2, 2008
    Publication date: January 8, 2009
    Applicant: LG Chem, Ltd.
    Inventors: Jun-seon Choi, Byoung-gi Park, Jin-do Kim, Hyune-jung Ryu
  • Publication number: 20080081008
    Abstract: The present invention relates to an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking, method for preparing the same and a method for preparing olefin by using the same. More precisely, the present invention relates to an oxide catalyst for hydrocarbon steam cracking represented by formula 1 and a phosphoric oxide catalyst for hydrocarbon steam cracking represented by formula 3 which would be used for the production of olefin such as ethylene and propylene by hydrocarbon steam cracking, and a method for preparing the same. The present invention provides an oxide catalyst and a phosphoric oxide catalyst for hydrocarbon steam cracking that has excellent thermo-stability at high temperature and improved olefin yield. CrZrjAkOx??[Formula 1] CrZrjAkPlOx??[Formula 3] Wherein, j, k, l and x are as indicated in the description.
    Type: Application
    Filed: September 24, 2007
    Publication date: April 3, 2008
    Applicants: LG CHEM, LTD., LG Petrochemical Co., Ltd.
    Inventors: Jun-seon Choi, Jun-Han Kang, Jong-hun Song, Byoung-gi Park, Chang-hoon Kang, Si-hyun Noh
  • Publication number: 20070053811
    Abstract: A hybrid adsorbent-membrane reactor in which the chemical reaction, membrane separation, and product adsorption are coupled. Also disclosed are a dual-reactor apparatus and a process using the reactor or the apparatus.
    Type: Application
    Filed: February 14, 2006
    Publication date: March 8, 2007