    Abstract: A method is used to make an aluminum alloy with excellent tensile strength, low density and excellent radiation. The method includes the steps of providing a base material, adding 0.06 wt % to 0.30 wt % of zirconium and 0.06 wt % to 0.30 wt % of vanadium to the base material, and melting the basic material with the zirconium and vanadium to provide an aluminum alloy. The base material includes 92.55 wt % to 97.38 wt % of aluminum, 0.9 wt % to 1.8 wt % of silicon, less than 0.5 wt % of iron, 0.6 wt % to 1.2 wt % of copper, 0.4 wt % to 1.1 wt % of manganese, 0.6 wt % to 1.4 wt % of magnesium, less than 0.40 wt % of chromium, less than 0.25 wt % of zinc and less than 0.20 wt % of titanium.
    Type: Application
    Filed: January 16, 2014
    Publication date: May 15, 2014
    Applicant: Chung-Shan Institute of Science and Technology, Armaments, Bureau, Ministry of National Defense
    Inventors: Chang-Chuan Hsu, Shan Torng, Sy-Cherng Yang, Fan-Chun Tseng, Wei-Ming Huang, Ren-An Luo
  • Publication number: 20130269480
    Abstract: A method is used to make an aluminum alloy with excellent tensile strength, low density and excellent radiation. The method includes the steps of providing a base material, adding 0.06 wt % to 0.30 wt % of zirconium and 0.06 wt % to 0.30 wt % of vanadium to the base material, and melting the basic material with the zirconium and vanadium to provide an aluminum alloy. The base material includes 92.55 wt % to 97.38 wt % of aluminum, 0.9 wt % to 1.8 wt % of silicon, less than 0.5 wt % of iron, 0.6 wt % to 1.2 wt % of copper, 0.4 wt % to 1.1 wt % of manganese, 0.6 wt % to 1.4 wt % of magnesium, less than 0.40 wt % of chromium, less than 0.25 wt % of zinc and less than 0.20 wt % of titanium.
    Type: Application
    Filed: April 16, 2012
    Publication date: October 17, 2013
    Applicant: Chung-Shan Institute of Science and Technology, Armaments, Bureau, Ministry of National Defense
    Inventors: Chang-Chuan Hsu, Shan Torng, Sy-Cherng Yang, Fan-Chun Tseng, Wei-Ming Huang, Ren-An Luo