  • Patent number: 12146845
    Abstract: A component residual stress testing platform based on neutron diffraction and experimental method thereof are provided, the testing platform includes a component support, a rotating mainshaft, a first thrust cylindrical roller bearing, a first cylindrical roller bearing, a bearing spacing sleeve, a second cylindrical roller bearing, a sleeve, and a first fixed baffle. The rotating mainshaft is disposed on the component support. The first thrust cylindrical roller bearing, the first cylindrical roller bearing, the bearing spacing sleeve and the second cylindrical roller bearing are sleeved on the rotating mainshaft, the sleeve is sleeved outside the first cylindrical roller bearing, the bearing spacing sleeve and the second cylindrical roller bearing, a component to be tested is sleeved on the sleeve. The testing platform can support, move, tilt and rotate the component to be tested in a process of a residual stress testing.
    Type: Grant
    Filed: September 5, 2022
    Date of Patent: November 19, 2024
    Assignees: NCS Testing Technology CO., LTD, Central Iron & Steel Research Institute Co., Ltd
    Inventors: Lixia Yang, Haizhou Wang, Lizhi Ren, Danqi Huang, Lei Zhao, Xuejing Shen, Dongling Li, Zongxin Liu, Changwang Zhu, Yang Wang, Yunhai Jia
  • Publication number: 20240105370
    Abstract: The present invention discloses a high-entropy soft magnetic alloy with 900 K high-temperature resistance, comprising Fe, Co, Ni, Si and Al, and the atomic percent of the alloy composition is expressed as FexCoyNizSimAln, wherein x=40%-80%, y=20%-60%, z=0-30%, m=0-20%, n=0-20%, and x+y+z+m+n=100%; the atomic percent of other doping elements is p=0-5%, and 0.5?m/n?3; the performance indexes of the material include: at room temperature, saturation magnetization Ms=90-150 emu/g, and coercive force Hc=0.1-15 Oe; and at 900 K, saturation magnetization Ms=70-130 emu/g, and coercive force Hc=0.1-25 Oe.
    Type: Application
    Filed: December 6, 2023
    Publication date: March 28, 2024
    Inventors: Haizhou Wang, Runqiu Lang, Haiyang Chen, Yandong Wang, Lei Zhao, Changwang Zhu, Xiaofen Zhang, Lixia Yang, Dongling Li, Xuejing Shen, Yunhai Jia
  • Publication number: 20230358693
    Abstract: A component residual stress testing platform based on neutron diffraction and experimental method thereof are provided, the testing platform includes a component support, a rotating mainshaft, a first thrust cylindrical roller bearing, a first cylindrical roller bearing, a bearing spacing sleeve, a second cylindrical roller bearing, a sleeve, and a first fixed baffle. The rotating mainshaft is disposed on the component support. The first thrust cylindrical roller bearing, the first cylindrical roller bearing, the bearing spacing sleeve and the second cylindrical roller bearing are sleeved on the rotating mainshaft, the sleeve is sleeved outside the first cylindrical roller bearing, the bearing spacing sleeve and the second cylindrical roller bearing, a component to be tested is sleeved on the sleeve. The testing platform can support, move, tilt and rotate the component to be tested in a process of a residual stress testing.
    Type: Application
    Filed: September 5, 2022
    Publication date: November 9, 2023
    Inventors: LIXIA YANG, HAIZHOU WANG, LIZHI REN, DANQI HUANG, LEI ZHAO, XUEJING SHEN, DONGLING LI, ZONGXIN LIU, CHANGWANG ZHU, YANG WANG, YUNHAI JIA