  • Patent number: 10851433
    Abstract: A martensitic stainless steel containing, by mass %, C: 0.20% to 0.40%, N: 0.1% or less, Mo: 3% or less, and Cr: 12.0% to 16.0%, such that 0.3%?C+N?0.4% and a PI value (=Cr+3.3Mo+16N) is 18 or more, with the remainder being substantially Fe and unavoidable impurities is quenched from a temperature of 1,030° C. to 1,140° C. and subjected to a subzero treatment and tempering so as to obtain a prior austenite crystal grain size of a surface layer of 30 ?m to 100 ?m and a surface hardness of 58 HRc to 62 HRc.
    Type: Grant
    Filed: December 13, 2018
    Date of Patent: December 1, 2020
    Assignee: NSK LTD.
    Inventors: Chikara Matsuzawa, Takafumi Yasuhara, Hiroshi Nishizawa, Norihiro Aoki, Koji Takano, Masaru Kuge
  • Patent number: 10494692
    Abstract: A martensitic stainless steel containing, by mass %, C: 0.20% to 0.40%, N: 0.1% or less, Mo: 3% or less, and Cr: 12.0% to 16.0%, such that 0.3%?C+N?0.4% and a PI value (=Cr+3.3Mo+16N) is 18 or more, with the remainder being substantially Fe and unavoidable impurities is quenched from a temperature of 1,030° C. to 1,140° C. and subjected to a subzero treatment and tempering so as to obtain a prior austenite crystal grain size of a surface layer of 30 ?m to 100 ?m and a surface hardness of 58 HRc to 62 HRc.
    Type: Grant
    Filed: November 13, 2014
    Date of Patent: December 3, 2019
    Assignee: NSK LTD.
    Inventors: Chikara Matsuzawa, Takafumi Yasuhara, Hiroshi Nishizawa, Norihiro Aoki, Koji Takano, Masaru Kuge
  • Publication number: 20190112686
    Abstract: A martensitic stainless steel containing, by mass %, C: 0.20% to 0.40%, N: 0.1% or less, Mo: 3% or less, and Cr: 12.0% to 16.0%, such that 0.3%?C+N?0.4% and a PI value (=Cr+3.3 Mo+16 N) is 18 or more, with the remainder being substantially Fe and unavoidable impurities is quenched from a temperature of 1,030° C. to 1,140° C. and subjected to a subzero treatment and tempering so as to obtain a prior austenite crystal grain size of a surface layer of 30 ?m to 100 ?m and a surface hardness of 58 HRc to 62 HRc.
    Type: Application
    Filed: December 13, 2018
    Publication date: April 18, 2019
    Applicant: NSK LTD.
    Inventors: Chikara MATSUZAWA, Takafumi YASUHARA, Hiroshi NISHIZAWA, Norihiro AOKI, Koji TAKANO, Masaru KUGE
  • Publication number: 20160289785
    Abstract: A martensitic stainless steel containing, by mass %, C: 0.20% to 0.40%, N: 0.1% or less, Mo: 3% or less, and Cr: 12.0% to 16.0%, such that 0.3%?C+N?0.4% and a PI value (=Cr+3.3Mo+16N) is 18 or more, with the remainder being substantially Fe and unavoidable impurities is quenched from a temperature of 1,030° C. to 1,140° C. and subjected to a subzero treatment and tempering so as to obtain a prior austenite crystal grain size of a surface layer of 30 ?m to 100 ?m and a surface hardness of 58 HRc to 62 HRc.
    Type: Application
    Filed: November 13, 2014
    Publication date: October 6, 2016
    Applicant: NSK LTD.
    Inventors: Chikara MATSUZAWA, Takafumi YASUHARA, Hiroshi NISHIZAWA, Norihiro AOKI, Koji TAKANO, Masaru KUGE