    Abstract: A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a first zone reaction product, the CTA system of the first reactor zone having a transfer activity Z1; and B. (1) Transferring at least part of the first zone reaction product to a second reactor zone selected from a second autoclave reactor zone or a tubular reactor zone and operating at polymerization conditions, and, optionally, (2) freshly injecting, a second feed into the second reactor zone to produce a second zone reaction product, with the proviso that at least one of the first reactor zone product and the freshly injected feed comprises a CTA system with a transfer activity of Z2; and with the proviso that the ratio of Z1:Z2 is greater than 1.
    Type: Grant
    Filed: December 28, 2015
    Date of Patent: January 3, 2017
    Assignee: Dow Global Technologies LLC
    Inventors: Otto J. Berbee, Cornelis F. J. den Doelder, Cornelis J. Hosman
  • Publication number: 20160115256
    Abstract: A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a first zone reaction product, the CTA system of the first reactor zone having a transfer activity Z1; and B. (1) Transferring at least part of the first zone reaction product to a second reactor zone selected from a second autoclave reactor zone or a tubular reactor zone and operating at polymerization conditions, and, optionally, (2) freshly injecting, a second feed into the second reactor zone to produce a second zone reaction product, with the proviso that at least one of the first reactor zone product and the freshly injected feed comprises a CTA system with a transfer activity of Z2; and with the proviso that the ratio of Z1:Z2 is greater than 1.
    Type: Application
    Filed: December 28, 2015
    Publication date: April 28, 2016
    Inventors: Otto J. Berbee, Cornelis F.J. de Doelder, Cornelis J. Hosman
  • Patent number: 9234055
    Abstract: A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a first zone reaction product, the CTA system of the first reactor zone having a transfer activity Z1; and B. (1) Transferring at least part of the first zone reaction product to a second reactor zone selected from a second autoclave reactor zone or a tubular reactor zone and operating at polymerization conditions, and, optionally, (2) freshly injecting, a second feed into the second reactor zone to produce a second zone reaction product, with the proviso that at least one of the first reactor zone product and the freshly injected feed comprises a CTA system with a transfer activity of Z2; and with the proviso that the ratio of Z1:Z2 is greater than 1.
    Type: Grant
    Filed: September 21, 2011
    Date of Patent: January 12, 2016
    Assignee: Dow Global Technologies LLC
    Inventors: Otto J. Berbee, Cornelis F. J. den Doelder, Cornelis J. Hosman
  • Patent number: 9120880
    Abstract: The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction zone that receives fresh ethylene, the ratio, Rn (n=reaction zone number, n>1), of “mass fraction of fresh ethylene fed to the first reaction zone (RZ1)” to “mass fraction of fresh ethylene fed to the nth reaction zone (RZn)” is (Rn=RZ1/RZn) greater than 1, or is from 0 to 0.
    Type: Grant
    Filed: October 10, 2012
    Date of Patent: September 1, 2015
    Assignee: Dow Global Technologies LLC
    Inventors: Werner Zschoch, Otto J. Berbee, Cornelis J. Hosman
  • Patent number: 8859704
    Abstract: Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
    Type: Grant
    Filed: April 8, 2013
    Date of Patent: October 14, 2014
    Assignee: Dow Global Technologies LLC
    Inventors: Teresa P. Karjala, Christopher R. Eddy, Mehmet Demirors, Wallace W. Yau, Sarat Munjal, Stefan Hinrichs, Jian Wang, Otto J. Berbee, Werner Zschoch, Cornelis J. Hosman, Lonnie G. Hazlitt
  • Publication number: 20140288257
    Abstract: The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction zone that receives fresh ethylene, the ratio, Rn (n=reaction zone number, n>1), of “mass fraction of fresh ethylene fed to the first reaction zone (RZ1)” to “mass fraction of fresh ethylene fed to the nth reaction zone (RZn)” is (Rn=RZ1/RZn) greater than 1, or is from 0 to 0.
    Type: Application
    Filed: October 10, 2012
    Publication date: September 25, 2014
    Applicant: Dow Global Technologies LLC
    Inventors: Werner Zschoch, Otto J. Berbee, Cornelis J. Hosman
  • Publication number: 20130197168
    Abstract: A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a first zone reaction product, the CTA system of the first reactor zone having a transfer activity Z1; and B. (1) Transferring at least part of the first zone reaction product to a second reactor zone selected from a second autoclave reactor zone or a tubular reactor zone and operating at polymerization conditions, and, optionally, (2) freshly injecting, a second feed into the second reactor zone to produce a second zone reaction product, with the proviso that at least one of the first reactor zone product and the freshly injected feed comprises a CTA system with a transfer activity of Z2; and with the proviso that the ratio of Z1:Z2 is greater than 1.
    Type: Application
    Filed: September 21, 2011
    Publication date: August 1, 2013
    Inventors: Otto J. Berbee, Cornelis F.J. den Doelder, Cornelis J. Hosman
  • Patent number: 8415442
    Abstract: Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
    Type: Grant
    Filed: October 1, 2009
    Date of Patent: April 9, 2013
    Assignee: Dow Global Technologies LLC
    Inventors: Teresa P. Karjala, Christopher R. Eddy, Mehmet Demirors, Wallace W. Yau, Sarat Munjal, Stefan Hinrichs, Jian Wang, Otto J. Berbee, Werner Zschoch, Cornelis J. Hosman, Lonnie G. Hazlitt
  • Publication number: 20110178253
    Abstract: Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
    Type: Application
    Filed: October 1, 2009
    Publication date: July 21, 2011
    Applicant: Dow Global Technologies LLC
    Inventors: Teresa P. Karjala, Christopher R. Eddy, Mehmet Demirors, Wallace W. Yau, Sarat Munjal, Stefan Hinrichs, Jian Wang, Otto J. Berbee, Werner Zschoch, Cornelis J. Hosman, Lonnie G. Hazlitt
  • Publication number: 20100087606
    Abstract: Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
    Type: Application
    Filed: October 2, 2009
    Publication date: April 8, 2010
    Inventors: Teresa P. Karjala, Christopher R. Eddy, Mehmet Demirors, Wallace W. Yau, Sarat Munjal, Stefan Hinrichs, Jian Wang, Otto J. Berbee, Werner Zschoch, Cornelis J. Hosman, Lonnie G. Hazlitt, John O. Osby