Patents by Inventor David J. Chaiko

David J. Chaiko has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 11898221
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the step of processing a metal sulfide concentrate in a reductive activation circuit 220 that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate. The method may further comprise the step of subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit 240 to extract metal values. In some disclosed embodiments, reductive activation steps and/or oxidative dissolution steps may employ mechano-chemical and/or physico-chemical processing of particles or agglomerates thereof. Reductive activation may be made prior to heap leaching or bio-leaching operations to improve metal extraction. Systems for practicing the aforementioned methods are also disclosed.
    Type: Grant
    Filed: August 13, 2020
    Date of Patent: February 13, 2024
    Inventors: David J. Chaiko, Frank Baczek, Sara (Sally) Rocks, Carlos Eyzaguirre
  • Patent number: 11124858
    Abstract: A method for removing sulfate iron-containing compounds from a low- to moderate-temperature metal sulfide leach circuit (1) is disclosed. A reactor (6) within a chloride leach circuit (5) and which is preferably maintained at a temperature between 20 and 150 degrees Celsius may be provided with a catalyst (4) comprising a material selected from the group consisting of: colloidal hematite, colloidal goethite, particulate containing FeOOH, particulate containing ?-FeOOH, particulate containing ?-FeOOH, particulate containing Fe2O3, particulate containing ?-Fe2O3, particulate containing ?-Fe2O3, particulate containing Fe3O4, particulate containing Fe(OH)SO4, and a combination thereof. The catalyst (4) may also be used with heap leach and/or dump leach circuits (22), without limitation. Methods for using and generating the catalyst (4) are also disclosed. In some embodiments, the catalyst (4) may be used as an anti-frothing agent (e.g., for zinc leaching, without limitation).
    Type: Grant
    Filed: August 27, 2019
    Date of Patent: September 21, 2021
    Inventor: David J. Chaiko
  • Patent number: 11124856
    Abstract: Systems for improving metal leach kinetics and metal recovery during atmospheric or substantially atmospheric leaching of a metal sulfide are disclosed. In some embodiments, an oxidative leach circuit 200 may employ Mechano-Chemcial/Physico-Chemical processing means for improving leach kinetics and/or metal recovery. In preferred embodiments, the Mechano-Chemcial/Physico-Chemical means comprises various combinations of stirred-tank reactors 202 and shear-tank reactors 212. As will be described herein, the stirred-tank reactors 202 and shear-tank reactors 212 may be arranged in series and/or in parallel with each other, without limitation. In some non-limiting embodiments, a shear-tank reactor 212 may also be disposed, in-situ, within a stirred-tank reactor 202.
    Type: Grant
    Filed: November 20, 2015
    Date of Patent: September 21, 2021
    Inventors: David J. Chaiko, Frank Baczek, Sara (Sally) Rocks, Carlos Eyzaguirre
  • Publication number: 20210246526
    Abstract: A method for removing sulfate iron-containing compounds from a low- to moderate-temperature metal sulfide leach circuit (1) is disclosed. A reactor (6) within a chloride leach circuit (5) and which is preferably maintained at a temperature between 20 and 150 degrees Celsius may be provided with a catalyst (4) comprising a material selected from the group consisting of: colloidal hematite, colloidal goethite, particulate containing FeOOH, particulate containing ?-FeOOH, particulate containing ?-FeOOH, particulate containing Fe2O3, particulate containing ?-Fe2O3, particulate containing ?-Fe2O3, particulate containing Fe3O4, particulate containing Fe(OH)SO4, and a combination thereof. The catalyst (4) may also be used with heap leach and/or dump leach circuits (22), without limitation. Methods for using and generating the catalyst (4) are also disclosed. In some embodiments, the catalyst (4) may be used as an anti-frothing agent (e.g., for zinc leaching, without limitation).
    Type: Application
    Filed: August 27, 2019
    Publication date: August 12, 2021
    Inventor: David J. Chaiko
  • Publication number: 20210062294
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the step of processing a metal sulfide concentrate in a reductive activation circuit 220 that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate. The method may further comprise the step of subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit 240 to extract metal values. In some disclosed embodiments, reductive activation steps and/or oxidative dissolution steps may employ mechano-chemical and/or physico-chemical processing of particles or agglomerates thereof. Reductive activation may be made prior to heap leaching or bio-leaching operations to improve metal extraction. Systems for practicing the aforementioned methods are also disclosed.
    Type: Application
    Filed: August 13, 2020
    Publication date: March 4, 2021
    Inventors: David J. Chaiko, Frank Baczek, Sara (Sally) Rocks, Carlos Eyzaguirre
  • Patent number: 10781501
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the step of processing a metal sulfide concentrate in a reductive activation circuit 220 that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate. The method may further comprise the step of subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit 240 to extract metal values. In some disclosed embodiments, reductive activation steps and/or oxidative dissolution steps may employ mechano-chemical and/or physico-chemical processing of particles or agglomerates thereof. Reductive activation may be made prior to heap leaching or bio-leaching operations to improve metal extraction. Systems for practicing the aforementioned methods are also disclosed.
    Type: Grant
    Filed: November 20, 2015
    Date of Patent: September 22, 2020
    Assignee: FLSmidth A/S
    Inventors: David J. Chaiko, Frank Baczek, Sara (Sally) Rocks, Carlos Eyzaguirre
  • Patent number: 10526681
    Abstract: A system and method for improving leach kinetics and recovery during above-atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of: (a) producing a metal sulfide concentrate [34] via flotation; (b) moving the produced metal sulfide concentrate [34] to at least one chamber [22a] of at least one reactor such as an autoclave [20]; (c) leaching the produced metal sulfide concentrate in said at least one chamber [22a] in the presence of oxygen [82] at a pressure and/or temperature above ambient, and in the presence of partially-used [25] and/or or new [92] grinding media within the at least one chamber [22a]. Systems [10] and apparatus [20, 200] for practicing the aforementioned method are also disclosed.
    Type: Grant
    Filed: December 16, 2015
    Date of Patent: January 7, 2020
    Assignee: FLSMIDTH A/S
    Inventors: David J. Chaiko, Carlos Eyzaguirre
  • Patent number: 10407753
    Abstract: A method of improving leach kinetics and recovery during atmospheric or above-atmospheric leaching of a metal sulfide is disclosed. A system for practicing the aforementioned method is also disclosed. Apparatus for practicing the aforementioned method is also disclosed. A new composition of matter which is formed by the aforementioned method, and which may be utilized in the system and apparatus is further disclosed. The new composition of matter may exhibit improved leach kinetics, and may have some utility in the semi-conductor arts, including uses within photovoltaic materials.
    Type: Grant
    Filed: December 21, 2015
    Date of Patent: September 10, 2019
    Assignee: FLSmidth A/S
    Inventors: David J. Chaiko, Sara (Sally) Rocks
  • Publication number: 20190100823
    Abstract: A system and method for improving leach kinetics and recovery during above-atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of: (a) producing a metal sulfide concentrate [34] via flotation; (b) moving the produced metal sulfide concentrate [34] to at least one chamber [22a] of at least one reactor such as an autoclave [20]; (c) leaching the produced metal sulfide concentrate in said at least one chamber [22a] in the presence of oxygen [82] at a pressure and/or temperature above ambient, and in the presence of partially-used [25] and/or or new [92] grinding media within the at least one chamber [22a]. Systems [10] and apparatus [20, 200] for practicing the aforementioned method are also disclosed.
    Type: Application
    Filed: December 16, 2015
    Publication date: April 4, 2019
    Inventors: David J. Chaiko, Carlos Eyzaguirre
  • Patent number: 10081849
    Abstract: A method of operating a concentrator may comprise producing a final copper concentrate and periodically or continuously analyzing the produced final copper concentrate to obtain a grade value of the produced final copper concentrate. The produced final copper concentrate may be sent to a downstream smelting operation if/when the grade value of the produced final copper concentrate is at or above a minimum acceptable grade threshold and may be sent to a downstream hydrometallurgical operation capable of producing copper cathode, if/when the grade value of the produced final copper concentrate is below or falls below the minimum acceptable grade threshold.
    Type: Grant
    Filed: August 11, 2015
    Date of Patent: September 25, 2018
    Assignee: FLSMIDTH A/S
    Inventors: David J. Chaiko, Gary Roy
  • Patent number: 10023935
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of: (a) producing a metal sulfide flotation concentrate; (b) processing the metal sulfide concentrate in a reductive activation circuit that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate; and, (c) subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit to extract metal values. In some disclosed embodiments, reductive activation steps may be employed prior to oxidative leaching steps (including heap leap leaching or bio-leaching steps). In some embodiments, physico-chemical processing steps may be employed during reductive activation and/or oxidative leaching. Systems for practicing the aforementioned methods are also disclosed.
    Type: Grant
    Filed: September 14, 2015
    Date of Patent: July 17, 2018
    Assignee: FLSmidth A/S
    Inventors: David J. Chaiko, Frank Baczek, Tom Walters, Sarah (Sally) Rocks, Carlos Eyzaguirre
  • Patent number: 10000389
    Abstract: A method of controlling frothing during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of (a) producing a metal sulfide concentrate via flotation; (b) producing a tailings stream via flotation; and, (c) diverting a portion or all of said produced tailings stream to an atmospheric or substantially atmospheric sulfide leach circuit. A metal recovery flowsheet is also disclosed. In some embodiments, the metal recovery flowsheet may comprise a unit operation comprising: (a) a sulfide concentrator comprising a flotation circuit, the flotation circuit producing a metal sulfide concentrate stream, and a tailings stream; and, (b) an atmospheric or substantially atmospheric metal sulfide leach circuit. The sulfide concentrator may be operatively connected to the atmospheric or substantially atmospheric metal sulfide leach circuit via both of said metal sulfide concentrate stream, and said tailings stream.
    Type: Grant
    Filed: August 27, 2015
    Date of Patent: June 19, 2018
    Assignee: FLSMIDTH A/S
    Inventors: David J. Chaiko, Frank Baczek, Tom Walters, Sarah (Sally) Rocks, Gary Roy, Carlos Eyzaguirre
  • Publication number: 20170369968
    Abstract: A method of improving leach kinetics and recovery during atmospheric or above-atmospheric leaching of a metal sulfide is disclosed. A system for practicing the aforementioned method is also disclosed. Apparatus for practicing the aforementioned method is also disclosed. A new composition of matter which is formed by the aforementioned method, and which may be utilized in the system and apparatus is further disclosed. The new composition of matter may exhibit improved leach kinetics, and may have some utility in the semi-conductor arts, including uses within photovoltaic materials.
    Type: Application
    Filed: December 21, 2015
    Publication date: December 28, 2017
    Inventors: David J. Chaiko, Sara (Sally) Rocks
  • Publication number: 20170356063
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the step of processing a metal sulfide concentrate in a reductive activation circuit 220 that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate. The method may further comprise the step of subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit 240 to extract metal values. In some disclosed embodiments, reductive activation steps and/or oxidative dissolution steps may employ mechano-chemical and/or physico-chemical processing of particles or agglomerates thereof. Reductive activation may be made prior to heap leaching or bio-leaching operations to improve metal extraction. Systems for practicing the aforementioned methods are also disclosed.
    Type: Application
    Filed: November 20, 2015
    Publication date: December 14, 2017
    Inventors: David J. Chaiko, Frank Baczek, Sara (Sally) Rocks, Carlos Eyzaguirre
  • Publication number: 20170283908
    Abstract: A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of: (a) producing a metal sulfide flotation concentrate; (b) processing the metal sulfide concentrate in a reductive activation circuit that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate; and, (c) subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit to extract metal values. In some disclosed embodiments, reductive activation steps may be employed prior to oxidative leaching steps (including heap leap leaching or bio-leaching steps). In some embodiments, physico-chemical processing steps may be employed during reductive activation and/or oxidative leaching. Systems for practicing the aforementioned methods are also disclosed.
    Type: Application
    Filed: September 14, 2015
    Publication date: October 5, 2017
    Inventors: David J. Chaiko, Frank Baczek, Tom Walters, Sarah (Sally) Rocks, Carlos Eyzaguirre
  • Publication number: 20170275177
    Abstract: A method of controlling frothing during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of (a) producing a metal sulfide concentrate via flotation; (b) producing a tailings stream via flotation; and, (c) diverting a portion or all of said produced tailings stream to an atmospheric or substantially atmospheric sulfide leach circuit. A metal recovery flowsheet is also disclosed. In some embodiments, the metal recovery flowsheet may comprise a unit operation comprising: (a) a sulfide concentrator comprising a flotation circuit, the flotation circuit producing a metal sulfide concentrate stream, and a tailings stream; and, (b) an atmospheric or substantially atmospheric metal sulfide leach circuit. The sulfide concentrator may be operatively connected to the atmospheric or substantially atmospheric metal sulfide leach circuit via both of said metal sulfide concentrate stream, and said tailings stream.
    Type: Application
    Filed: August 27, 2015
    Publication date: September 28, 2017
    Inventors: David J. Chaiko, Frank Baczek, Tom Walters, Sarah (Sally) Rocks, Gary Roy, Carlos Eyzaguirre
  • Publication number: 20170226611
    Abstract: A method of operating a copper or other metal value concentrator is disclosed. According to some embodiments, the method may comprise producing a final copper concentrate; periodically or continuously analyzing the produced final copper concentrate to obtain a grade value of the produced final copper concentrate; and diverting the produced final copper concentrate to a downstream smelting operation if/when the grade value of the produced final copper concentrate is at or above a minimum acceptable grade threshold; or, diverting the produced final copper concentrate to a downstream hydrometallurgical operation capable of producing copper cathode or other saleable copper product from the produced final copper concentrate, if/when the grade value of the produced final copper concentrate is below said minimum acceptable grade threshold. A copper concentrator capable of conducting the aforementioned method steps is also disclosed.
    Type: Application
    Filed: August 11, 2015
    Publication date: August 10, 2017
    Inventors: David J. Chaiko, Gary Roy
  • Publication number: 20170080355
    Abstract: A mixer settler system is disclosed. The system comprises a mixer [110] configured for receiving an organic phase and an aqueous phase, the mixer [110] being further configured to maintain the organic phase and the aqueous phase in a single unstable emulsion phase, wherein mass transfer occurs between said organic phase and said aqueous phase; and, a column settler [120] which is configured to receive a single unstable emulsion phase from the mixer [110] via an emulsion inlet [125] and is also configured to separate the single unstable emulsion phase into a stable organic phase and a stable aqueous phase by virtue of coalescence; the column settler further comprising an organic outlet [121] above the emulsion inlet [125] and an aqueous outlet [123] below the emulsion inlet [125]; the column settler [120] further discouraging mass transfers within the unstable emulsion phase and further promoting coalescence of each of said stable organic phase and stable aqueous phase.
    Type: Application
    Filed: February 16, 2015
    Publication date: March 23, 2017
    Inventors: Frank Baczek, David J. Chaiko, Vishal Gupta, Suma Kandagatla, Bryan Potratz, Gary Roy
  • Patent number: 9422610
    Abstract: Disclosed are novel compounds which display enhanced reactive properties due, in part, to induced lattice strain. The new compounds demonstrate accelerated leaching of copper under oxidizing conditions. The activated compounds are produced under conditions of time, temperature, Eh, and pH which retard the rate of lattice strain relaxation. Further disclosed are methods of making and using the novel compounds.
    Type: Grant
    Filed: January 11, 2016
    Date of Patent: August 23, 2016
    Assignee: FLSmidth A/S
    Inventors: David J. Chaiko, Sara (Sally) Rocks
  • Publication number: 20160201162
    Abstract: Disclosed are novel compounds which display enhanced reactive properties due, in part, to induced lattice strain. The new compounds demonstrate accelerated leaching of copper under oxidizing conditions. The activated compounds are produced under conditions of time, temperature, Eh, and pH which retard the rate of lattice strain relaxation. Further disclosed are methods of making and using the novel compounds.
    Type: Application
    Filed: January 11, 2016
    Publication date: July 14, 2016
    Inventors: David J. Chaiko, Sara (Sally) Rocks