  • Publication number: 20110104383
    Abstract: The present invention is directed to a method for protecting metal surfaces in oil & gas exploration and production, refinery and petrochemical process applications subject to solid particulate erosion at temperatures of up to 1000° C. The method includes the step of providing the metal surfaces in such applications with a hot erosion resistant cermet lining or insert, wherein the cermet lining or insert includes a) about 30 to about 95 vol % of a ceramic phase, and b) a metal binder phase, wherein the cermet lining or insert has a HEAT erosion resistance index of at least 5.0 and a K1C fracture toughness of at least 7.0 MPa-m1/2. The metal surfaces may also be provided with a hot erosion resistant cermet coating having a HEAT erosion resistance index of at least 5.0.
    Type: Application
    Filed: October 26, 2010
    Publication date: May 5, 2011
    Applicant: EXXONMOBIL RESEARCH AND ENGINEERING COMPANY
    Inventors: JOHN ROGER PETERSON, NARASIMHA-RAO V. BANGARU, ROBERT LEE ANTRAM, CHRISTOPHER JOHN FOWLER, NEERAJ S. THIRUMALAI, CHANGMIN CHUN, EMERY B. LENDVAI-LINTNER
  • Publication number: 20110104384
    Abstract: The present invention is directed to a method for protecting metal surfaces in oil & gas exploration and production, refinery and petrochemical process applications subject to solid particulate erosion at temperatures of up to 1000° C. The method includes the step of providing the metal surfaces in such applications with a hot erosion resistant cermet lining or insert, wherein the cermet lining or insert includes a) about 30 to about 95 vol % of a ceramic phase, and b) a metal binder phase, wherein the cermet lining or insert has a HEAT erosion resistance index of at least 5.0 and a K1C fracture toughness of at least 7.0 MPa-m1/2. The metal surfaces may also be provided with a hot erosion resistant cermet coating having a HEAT erosion resistance index of at least 5.0.
    Type: Application
    Filed: October 26, 2010
    Publication date: May 5, 2011
    Applicant: ExxonMobil Research and Engineering Company
    Inventors: John R. Peterson, Narasimha-Rao V. Bangaru, Robert Lee Antram, Christopher John Fowler, Neeraj S. Thirumalai, ChangMin Chun, Emery B. Lendvai-Lintner
  • Publication number: 20110094627
    Abstract: The present invention is directed to a method for protecting metal surfaces in oil & gas exploration and production, refinery and petrochemical process applications subject to solid particulate erosion at temperatures of up to 1000° C. The method includes the step of providing the metal surfaces in such applications with a hot erosion resistant cermet lining or insert, wherein the cermet lining or insert includes a) about 30 to about 95 vol % of a ceramic phase, and b) a metal binder phase, wherein the cermet lining or insert has a HEAT erosion resistance index of at least 5.0 and a K1C fracture toughness of at least 7.0 MPa-m1/2. The metal surfaces may also be provided with a hot erosion resistant cermet coating having a HEAT erosion resistance index of at least 5.0.
    Type: Application
    Filed: October 26, 2010
    Publication date: April 28, 2011
    Applicant: ExxonMobil Research and Engineering Company
    Inventors: John R. Peterson, Narasimha-Rao V. Bangaru, Robert Lee Antram, Christopher John Fowler, Neeraj S. Thirumalai, ChangMin Chun, Emery B. Lendvai-Lintner
  • Patent number: 7842139
    Abstract: The present invention is directed to a method for protecting metal surfaces in oil & gas exploration and production, refinery and petrochemical process applications subject to solid particulate erosion at temperatures of up to 1000° C. The method includes the step of providing the metal surfaces in such applications with a hot erosion resistant cermet lining or insert, wherein the cermet lining or insert includes a) about 30 to about 95 vol % of a ceramic phase, and b) a metal binder phase, wherein the cermet lining or insert has a HEAT erosion resistance index of at least 5.0 and a K1C fracture toughness of at least 7.0 MPa-m1/2. The metal surfaces may also be provided with a hot erosion resistant cermet coating having a HEAT erosion resistance index of at least 5.0.
    Type: Grant
    Filed: June 30, 2006
    Date of Patent: November 30, 2010
    Assignee: ExxonMobil Research and Engineering Company
    Inventors: John R. Peterson, Narasimha-Rao V. Bangaru, Robert Lee Antram, Christopher John Fowler, Neeraj S. Thirumalai, ChangMin Chun, Emery B. Lendvai-Lintner
  • Patent number: 7731776
    Abstract: Multimodal cermet compositions comprising a multimodal grit distribution of the ceramic phase and method of making are provided by the present invention. The multimodal cermet compositions include a) a ceramic phase and b) a metal binder phase, wherein the ceramic phase is a metal boride with a multimodal distribution of particles, wherein at least one metal is selected from the group consisting of Group IV, Group V, Group VI elements of the Long Form of The Periodic Table of Elements and mixtures thereof, and wherein the metal binder phase comprises at least one first element selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, and at least second element selected from the group consisting of Cr, Al, Si and Y, and Ti.
    Type: Grant
    Filed: December 2, 2005
    Date of Patent: June 8, 2010
    Assignee: ExxonMobil Research and Engineering Company
    Inventors: ChangMin Chun, Narasimha-Rao V. Bangaru, Neeraj S. Thirumalai, Hyun-Woo Jin, Jayoung Koo, John R. Peterson, Robert L. Antram, Christopher J. Fowler, Emery B. Lendvai-Lintner
  • Publication number: 20080003125
    Abstract: The present invention is directed to a method for protecting metal surfaces in oil & gas exploration and production, refinery and petrochemical process applications subject to solid particulate erosion at temperatures of up to 1000° C. The method includes the step of providing the metal surfaces in such applications with a hot erosion resistant cermet lining or insert, wherein the cermet lining or insert includes a) about 30 to about 95 vol % of a ceramic phase, and b) a metal binder phase, wherein the cermet lining or insert has a HEAT erosion resistance index of at least 5.0 and a K1C fracture toughness of at least 7.0 MPa-m 1/2. The metal surfaces may also be provided with a hot erosion resistant cermet coating having a HEAT erosion resistance index of at least 5.0.
    Type: Application
    Filed: June 30, 2006
    Publication date: January 3, 2008
    Inventors: John R. Peterson, Narasimha-Rao V. Bangaru, Robert Lee Antram, Christopher John Fowler, Neeraj S. Thirumalai, ChangMin Chun, Emery B. Lendvai-Lintner