  • Patent number: 9216520
    Abstract: Process for the manufacture of a rubber composition comprising various constituents, such as base elastomers, reinforcing fillers, additives and a vulcanization system, during which the following stages are carried out: A—using a continuous mixing device, a starting rubber composition comprising the reinforcing fillers and optionally other components, with the exception of the crosslinking system, is produced, the operating parameters for the continuous mixing device being chosen so that: a—the residence time of the elastomer in the mixing chamber is between 20 and 60 seconds, b—the specific energy conferred on the rubber composition is between 2000 joules/gram and 5000 joules/gram, B—at the outlet for the starting rubber composition from the mixing chamber, the temperature of the said starting rubber composition is lowered to a temperature of less than 140° C. in less than 5 minutes.
    Type: Grant
    Filed: March 4, 2011
    Date of Patent: December 22, 2015
    Assignees: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN, Michelin Recherche et Technique S.A.
    Inventors: Jean-Marc Loubaresse, Floriandre Voisin, Pierre Annet, Bruno Dussardier, Gérald Huguenot, Arnaud Lapra, Julien Loyau, Vincent Pelissier
  • Patent number: 9023938
    Abstract: Method for the production of an initial rubber composition, in the course of which the following steps are carried out in succession: A—a rubber matrix, reinforcing fillers, and other components if required, with the exception of the cross-linking system, are introduced into a mixing means of the internal mixer type, comprising a mixing chamber in which there are mounted rotors which are driven in rotation and have radial projections forming a gap (e) between themselves and the vessel, B—said components are mixed in the chamber until a uniform mixture is obtained, care being taken to ensure that the temperature of the mixture remains at or below 170° C., after which C—the rotation speed of the rotors is adjusted so as to bring the rubber composition to a dropping temperature in the range from 180° C. to 240° C.
    Type: Grant
    Filed: July 25, 2012
    Date of Patent: May 5, 2015
    Assignees: Compagnie Generale des Etablissements Michelin, Michelin Recherche et Technique, S.A.
    Inventors: Jean-Marc Loubaresse, Marie Eloy, Floriandre Voisin, Gérald Huguenot, Julien Loyau
  • Publication number: 20140200307
    Abstract: Method for the production of an initial rubber composition, in the course of which the following steps are carried out in succession: A—a rubber matrix, reinforcing fillers, and other components if required, with the exception of the cross-linking system, are introduced into a mixing means of the internal mixer type, comprising a mixing chamber in which there are mounted rotors which are driven in rotation and have radial projections forming a gap (e) between themselves and the vessel, B—said components are mixed in the chamber until a uniform mixture is obtained, care being taken to ensure that the temperature of the mixture remains at or below 170° C., after which C—the rotation speed of the rotors is adjusted so as to bring the rubber composition to a dropping temperature in the range from 180° C. to 240° C.
    Type: Application
    Filed: July 25, 2012
    Publication date: July 17, 2014
    Applicant: MICHELIN RECHERCHE ET TECHNIQUE S.A.
    Inventors: Jean-Marc Loubaresse, Marie Eloy, Floriandre Voisin, Gérald Huguenot, Julien Loyau
  • Publication number: 20130203892
    Abstract: Process for the manufacture of a rubber composition comprising various constituents, such as base elastomers, reinforcing fillers, additives and a vulcanization system, during which the following stages are carried out: A—using a continuous mixing device, a starting rubber composition comprising the reinforcing fillers and optionally other components, with the exception of the crosslinking system, is produced, the operating parameters for the continuous mixing device being chosen so that: a—the residence time of the elastomer in the mixing chamber is between 20 and 60 seconds, b—the specific energy conferred on the rubber composition is between 2000 joules/gram and 5000 joules/gram, B—at the outlet for the starting rubber composition from the mixing chamber, the temperature of the said starting rubber composition is lowered to a temperature of less than 140° C. in less than 5 minutes.
    Type: Application
    Filed: March 4, 2011
    Publication date: August 8, 2013
    Applicant: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Jean-Marc Loubaresse, Floriandre Voisin, Pierre Annet, Bruno Dussardier, Gérald Huguenot, Arnaud Lapra, Julien Loyau, Vincent Pelissier