    Abstract: Provided are a method and apparatus for refining titanium scraps and sponge titanium, which can remove oxygen from a melt by supplying a deoxidizing gas to the surface of the melt in order to refine titanium scraps and sponge titanium. The method for refining titanium scraps and sponge titanium comprises supplying hydrogen ions and electrons in plasma to a titanium melt to remove oxygen from the titanium melt surface having an oxide layer formed thereon. In addition, the apparatus comprises: a vacuum chamber; a crucible located in the vacuum chamber and configured to perform melting by the magnetic field of an induction coil in a state in which a melt and the inner wall of the crucible; a calcium gas supply means configured to supply calcium gas from the bottom of the crucible to the space between the inner wall of the crucible and the melt.
    Type: Grant
    Filed: June 12, 2013
    Date of Patent: December 12, 2017
    Assignee: KOREA INSTITUTE OF INDUSTRIAL TECHNOLOGY
    Inventors: Byung Moon Moon, Gang June Kim, Jae Yoon Lee
  • Publication number: 20160177418
    Abstract: Provided are a method and apparatus for refining titanium scraps and sponge titanium, which can remove oxygen from a melt by supplying a deoxidizing gas to the surface of the melt in order to refine titanium scraps and sponge titanium. The method for refining titanium scraps and sponge titanium comprises supplying hydrogen ions and electrons in plasma to a titanium melt to remove oxygen from the titanium melt surface having an oxide layer formed thereon. In addition, the apparatus comprises: a vacuum chamber; a crucible located in the vacuum chamber and configured to perform melting by the magnetic field of an induction coil in a state in which a melt and the inner wall of the crucible; a calcium gas supply means configured to supply calcium gas from the bottom of the crucible to the space between the inner wall of the crucible and the melt.
    Type: Application
    Filed: June 12, 2013
    Publication date: June 23, 2016
    Applicant: Korea Institute of Industrial Technology
    Inventors: Byung Moon MOON, Gang June KIM, Jae Yoon LEE
  • Patent number: 9352970
    Abstract: In order to produce metallurgical grade silicon and solar cell grade polysilicon in batches, a method of the present invention comprises: a step of reduction in an arc furnace, consisting of removing C and CO in a silicon reduction atmosphere using silica stone and carbon black by an arc so as to produce metallurgical grade silicon; a step of refining by slag consisting of removing phosphorus (P) and boron (B) by slag; a step of refining by unidirectional solidification consisting of removing metal impurities (Fe, Al, Ti, Mn, etc.) by means of unidirectional solidification; and a step of steam plasma-electromagnetism continuous refining consisting of charging a furnace with the unidirectionally solidified silicon and removing boron (B) by a steam plasma torch.
    Type: Grant
    Filed: June 28, 2012
    Date of Patent: May 31, 2016
    Assignee: KOREA INSTITUTE OF INDUSTRIAL TECHNOLOGY
    Inventors: Byung Moon Moon, Tae U Yu, Dong Ho Park, Hyun Jin Koo, Gang June Kim, Eun Su Jang, Sang Wook Lee
  • Publication number: 20150135770
    Abstract: In order to produce metallurgical grade silicon and solar cell grade polysilicon in batches, a method of the present invention comprises: a step of reduction in an arc furnace, consisting of removing C and CO in a silicon reduction atmosphere using silica stone and carbon black by an arc so as to produce metallurgical grade silicon; a step of refining by slag consisting of removing phosphorus (P) and boron (B) by slag; a step of refining by unidirectional solidification consisting of removing metal impurities (Fe, Al, Ti, Mn, etc.) by means of unidirectional solidification; and a step of steam plasma-electromagnetism continuous refining consisting of charging a furnace with the unidirectionally solidified silicon and removing boron (B) by a steam plasma torch.
    Type: Application
    Filed: June 28, 2012
    Publication date: May 21, 2015
    Applicant: KOREA INSTITUTE OF INDUSTRIAL TECHNOLOGY
    Inventors: Byung Moon Moon, Tae U Yu, Dong Ho Park, Hyun Jin Koo, Gang June Kim, Eun Su Jang, Sang Wook Lee