  • Patent number: 7744806
    Abstract: As a first aspect, the present invention is directed to a process for making a heat-shrinkable annular film, comprising: (A) extruding an annular extrudate downward from an annular die; (B) quenching the annular extrudate by applying a quenching liquid to the annular extrudate; (C) reheating the extrudate to an orientation temperature of from 130° F. to 210° F., resulting in a reheated annular extrudate; and (D) orienting the reheated annular extrudate while the reheated annular extrudate is in the solid state, the orientation being carried out with a total orientation factor of at least 2, so that the resulting oriented, heat-shrinkable film has a total free shrink at 185° F. of at least 10 percent. The extrudate comprises at least one semi-crystalline polyamide selected from the group consisting of: (i) polyamide 6, (ii) polyamide 66, (iii) polyamide 6/66, and (iv) polyamide 6/12. The semi-crystalline polyamide makes up at least 5 volume percent of the annular extrudate.
    Type: Grant
    Filed: January 29, 2007
    Date of Patent: June 29, 2010
    Assignee: Cryovac, Inc.
    Inventors: Michael E. Broadus, Richard M. Dayrit, Bryan E. Freeman, Frank M. Hofmeister, Brian P. Rivers, Roger D. Vrooman, Christopher K. Robinson, George D. Bolden, Robert W. Campbell, Nathanael R. Miranda
  • Publication number: 20080179780
    Abstract: As a first aspect, the present invention is directed to a process for making a heat-shrinkable annular film, comprising: (A) extruding an annular extrudate downward from an annular die; (B) quenching the annular extrudate by applying a quenching liquid to the annular extrudate; (C) reheating the extrudate to an orientation temperature of from 130° F. to 210° F., resulting in a reheated annular extrudate; and (D) orienting the reheated annular extrudate while the reheated annular extrudate is in the solid state, the orientation being carried out with a total orientation factor of at least 2, so that the resulting oriented, heat-shrinkable film has a total free shrink at 185° F. of at least 10 percent. The extrudate comprises at least one semi-crystalline polyamide selected from the group consisting of: (i) polyamide 6, (ii) polyamide 66, (iii) polyamide 6/66, and (iv) polyamide 6/12. The semi-crystalline polyamide makes up at least 5 volume percent of the annular extrudate.
    Type: Application
    Filed: January 29, 2007
    Publication date: July 31, 2008
    Inventors: Michael E. Broadus, Richard M. Dayrit, Bryan E. Freeman, Frank M. Hofmeister, Brian P. Rivers, Roger D. Vrooman, Christopher K. Robinson, George D. Bolden, Robert W. Campbell, Nathanael R. Miranda