  • Publication number: 20130338051
    Abstract: The present invention provides a method for producing a chemically strengthened glass for a display device, which is capable of suppressing generation of concave defects. The present invention relates to a method for producing a chemically strengthened glass substrate for a display device, in which a calcium concentration in a cleaning liquid used in a final cleaning step before a chemical strengthening step is 5 ppm or less.
    Type: Application
    Filed: June 3, 2013
    Publication date: December 19, 2013
    Applicant: ASAHI GLASS COMPANY, LIMITED
    Inventors: Shuji Matsumoto, Tsuguhide Isemura, Koji Nakagawa, Kazutaka Ono, Shusaku Akiba, Haruo Aizawa
  • Publication number: 20120240626
    Abstract: The present invention relates to a process for producing a chemically strengthened glass substrate for a display device, the process including a pre-heating step of pre-heating a glass to a pre-heating temperature and subsequently an ion exchange step of immersing the glass in a chemical strengthening liquid, in which the pre-heating temperature in the pre-heating step and a strain point of the glass satisfy: 220° C.?(strain point?pre-heating temperature).
    Type: Application
    Filed: March 23, 2012
    Publication date: September 27, 2012
    Applicant: Asahi Glass Company, Limited
    Inventors: Syuji MATSUMOTO, Tsuguhide Isemura, Koji Nakagawa, Kazutaka Ono, Shusaku Akiba, Haruo Aizawa
  • Patent number: 5780373
    Abstract: A glass composition comprising from 45 to 66 wt % of SiO.sub.2, from 0 to 15 wt % of Al.sub.2 O.sub.3, from 10 to 24 wt % of Li.sub.2 O+Na.sub.2 O+K.sub.2 O, from 14 to 26 wt % of CaO+MgO+SrO+BaO+ZnO, and from 0 to 1 wt % of SO.sub.3 +Sb.sub.2 O.sub.3, said glass composition containing substantially no zirconia and having a strain point of at least 560.degree. C. and a linear thermal expansion coefficient of at least 80.times.10.sup.-7 /.degree.C. within a temperature range of from 50.degree. to 350.degree. C.
    Type: Grant
    Filed: December 20, 1996
    Date of Patent: July 14, 1998
    Assignee: Asahi Glass Company Ltd.
    Inventors: Osamu Yanagisawa, Kenji Oda, Naoki Sugimoto, Yoshio Takegawa, Akira Takada, Hideyo Osada, Haruo Aizawa, Koji Miura
  • Patent number: 5631195
    Abstract: A glass composition comprising from 45 to 66 wt % of SiO.sub.2, from 0 to 15 wt % of Al.sub.2 O.sub.3, from 10 to 24 wt % of Li.sub.2 O+Na.sub.2 O+K.sub.2 O, from 14 to 26 wt % of CaO+MgO+SrO+BaO+ZnO, and from 0 to 1 wt % of SO.sub.3 +Sb.sub.2 O.sub.3, said glass composition containing substantially no zirconia and having a strain point of at least 560.degree. C. and a linear thermal expansion coefficient of at least 80.times.10.sup.-7 /.degree.C. within a temperature range of from 50.degree. to 350.degree. C.
    Type: Grant
    Filed: September 14, 1995
    Date of Patent: May 20, 1997
    Assignee: Asahi Glass Company Ltd.
    Inventors: Osamu Yanagisawa, Kenji Oda, Naoki Sugimoto, Yoshio Takegawa, Akira Takada, Hideyo Osada, Haruo Aizawa, Koji Miura