  • Patent number: 9284475
    Abstract: Pressure sensitive adhesive composition and multilayer easy peel re-closable structures thereof, comprising a butene-1 (co)polymer (A) having a content of butene-1 derived units of 80 wt % or more; a flexural modulus (MEF) of 80 MPa or less; a melting temperature DSC (TmI) lower than 110° C., and optionally a tackifier (B).
    Type: Grant
    Filed: October 18, 2011
    Date of Patent: March 15, 2016
    Assignee: Basell Poliolefine Italia S.r.l.
    Inventors: Gianluca Musacchi, Inge Elisabeth Roucourt, Giampaolo Pellegatti, Johan De Clippeleir, Stefano Spataro
  • Publication number: 20130202836
    Abstract: Pressure sensitive adhesive composition and multilayer easy peel re-closable structures thereof, comprising a butene-1 (co)polymer (A) having a content of butene-1 derived units of 80 wt % or more; a flexural modulus (MEF) of 80 MPa or less; a melting temperature DSC (TmI) lower than 110° C., and optionally a tackifier (B).
    Type: Application
    Filed: October 18, 2011
    Publication date: August 8, 2013
    Applicant: Basell Poliolefine Italia S.r.I.
    Inventors: Gianluca Musacchi, Inge Elisabeth Roucourt, Giampaolo Pellegatti, Johan De Clippeleir, Stefano Spataro
  • Publication number: 20120171405
    Abstract: Film or sheet comprising at least one layer of a polyolefin composition consisting, in percentage by weight referred to the sum of component (a1) and (a2) and (b), of: a1) 42-88 wt % of a propylene homopolymer or copolymer of propylene with ethylene and/or one or more C4-C10 ?-olefin(s), the said homopolymer or copolymer having a solubility in xylene at room temperature (XSm) equal to or less than 10 wt %; a2) 7-39 wt % of a copolymer of ethylene with propylene and/or one or more C4-C10 ?-olefin(s) containing 50-80 wt % of ethylene derived units and having a solubility in xylene at room temperature of 50-80 wt %; and (b) 0.5-30 wt %, of a butene-1 (co)polymer having: a content of butene-1 derived units of 75 wt % or more, a flexural modulus (MEF) of 70 MPa or less.
    Type: Application
    Filed: September 15, 2010
    Publication date: July 5, 2012
    Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
    Inventors: Stefano Pasquali, Gianluca Musacchi, Enrico Beccarini, Inge Elisabeth Roucourt