Patent number: 7036707Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: July 2, 2003Date of Patent: May 2, 2006Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6936332Abstract: The friction stir welding technique disclosed avoids occurrence of a dent in adjoining region extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, thickened parts, which project toward the rotary body joining tool, are provided. The Two adjoining thickened parts form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion, and is inserted in the thickened parts. When the rotary body joining tool has been inserted small-diameter tip end first to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out. After the joining, the remaining parts of the thickened parts can be machined to form a smooth surface.Type: GrantFiled: April 10, 2001Date of Patent: August 30, 2005Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6722286Abstract: In a railway car, extruded frame members of an aluminum base alloy containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % are welded according to a friction stir welding method. In a structure, an aluminum base alloy plate containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % is prepared, to one face of the aluminum base alloy plate a rib is formed, and the aluminum base alloy plate is an extruded frame member. Accordingly, a railway car having a low welding distortion and a structure having a low welding distortion can be obtained.Type: GrantFiled: July 5, 2002Date of Patent: April 20, 2004Assignee: Hitachi, Ltd.Inventors: Hisanori Okamura, Isao Funyuu, Akihiro Satou, Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru
-
Patent number: 6716538Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: March 13, 2002Date of Patent: April 6, 2004Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20040004109Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: ApplicationFiled: July 2, 2003Publication date: January 8, 2004Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6640515Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 11, 2000Date of Patent: November 4, 2003Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6619534Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces, structural body formed. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region.Type: GrantFiled: July 3, 2002Date of Patent: September 16, 2003Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6613447Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces, structural body formed. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region.Type: GrantFiled: May 28, 2002Date of Patent: September 2, 2003Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6607837Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: March 13, 2002Date of Patent: August 19, 2003Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6585443Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 10, 2001Date of Patent: July 1, 2003Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20030005852Abstract: In a railway car, extruded frame members of an aluminum base alloy containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % are welded according to a friction stir welding method. In a structure, an aluminum base alloy plate containing Si of 0.4-0.9 wt % and Mg of 0.4-1.2 wt % is prepared, to one face of the aluminum base alloy plate a rib is formed, and the aluminum base alloy plate is an extruded frame member. Accordingly, a railway car having a low welding distortion and a structure having a low welding distortion can be obtained.Type: ApplicationFiled: July 5, 2002Publication date: January 9, 2003Inventors: Hisanori Okamura, Isao Funyuu, Akihiro Satou, Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru
-
Publication number: 20020162876Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces, structural body formed. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region.Type: ApplicationFiled: July 3, 2002Publication date: November 7, 2002Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20020139831Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces, structural body formed. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region.Type: ApplicationFiled: May 28, 2002Publication date: October 3, 2002Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20020094446Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: ApplicationFiled: March 13, 2002Publication date: July 18, 2002Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6419144Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 10, 2001Date of Patent: July 16, 2002Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20020090526Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: ApplicationFiled: March 13, 2002Publication date: July 11, 2002Inventors: Kinya Aota, Masakumi Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6382498Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 10, 2001Date of Patent: May 7, 2002Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6378754Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 10, 2001Date of Patent: April 30, 2002Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Patent number: 6305866Abstract: A friction stir welding technique which avoids occurrence of a dent, in a joining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip end first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: GrantFiled: April 11, 2000Date of Patent: October 23, 2001Assignee: Hitachi, Ltd.Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou
-
Publication number: 20010011670Abstract: Disclosed is a friction stir welding technique which avoids occurrence of a dent, in adjoining region, extending to a level beneath the joined surfaces. At end portions of the frame members to be joined, at the joining region, thickened parts which project toward the rotary body joining tool are provided. Two adjoining thickened parts, of adjacent members to be joined, can form a trapezoid shape. The rotary body joining tool has a small-diameter tip portion and a larger diameter portion. The rotary body joining tool is inserted in the thickened parts. In a state where the rotary body joining tool has been inserted small-diameter tip and first, to a level where the larger diameter portion of the rotary body joining tool overlaps the thickened part but does not extend below the upper surface of the non-thickened surfaces of the members joined, the rotary body is rotated and moved along the joining region. Even when a gap exists between two thickened parts, a desirable joining can be carried out.Type: ApplicationFiled: April 10, 2001Publication date: August 9, 2001Inventors: Kinya Aota, Masakuni Ezumi, Yasuo Ishimaru, Hisanori Okamura, Isao Funyuu, Akihiro Satou