  • Patent number: 10793760
    Abstract: A method and composition for modifying bentonite to allow the bentonite to be useful in drilling mud applications. The method includes the steps of: preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite; grinding the bentonite to a fine powder; sieving the fine powder to be between about 50 ?m and about 150 ?m in particle size to produce a sieved fine powder; mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition; adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and allowing the homogeneous solution of modified bentonite in water to rest for about 16 hours to form a composition useful in drilling mud applications.
    Type: Grant
    Filed: August 17, 2018
    Date of Patent: October 6, 2020
    Assignee: SAUDI ARABIAN OIL COMPANY
    Inventors: Mansour A. Al-Shafei, Akram A. Alfliow, Awad M. Al-Mofleh, Jamal M. Al-Aamri, Syed Rehan Ahmad Zaidi, Amer A. Al-Tuwailib
  • Publication number: 20180355235
    Abstract: A method and composition for modifying bentonite to allow the bentonite to be useful in drilling mud applications. The method includes the steps of: preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite; grinding the bentonite to a fine powder; sieving the fine powder to be between about 50 ?m and about 150 ?m in particle size to produce a sieved fine powder; mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition; adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and allowing the homogeneous solution of modified bentonite in water to rest for about 16 hours to form a composition useful in drilling mud applications.
    Type: Application
    Filed: August 17, 2018
    Publication date: December 13, 2018
    Applicant: Saudi Arabian Oil Company
    Inventors: Mansour A. Al-Shafei, Akram A. Alfliow, Awad M. Al-Mofleh, Jamal M. Al-Aamri, Syed Rehan Ahmad Zaidi, Amer A. Al-Tuwailib
  • Patent number: 10081751
    Abstract: Disclosed is a method for modifying bentonite to allow the bentonite to be useful in drilling mud applications. The method includes the steps of: preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite; grinding the bentonite to a fine powder; sieving the fine powder to be between about 50 ?m and about 150 ?m in particle size to produce a sieved fine powder; mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition; adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and allowing the homogeneous solution of modified bentonite in water to rest for about 16 hours to form a composition useful in drilling mud applications.
    Type: Grant
    Filed: April 1, 2016
    Date of Patent: September 25, 2018
    Assignee: Saudi Arabian Oil Company
    Inventors: Mansour A. Al-Shafei, Akram A. Alfliow, Awad M. Al-Mofleh, Jamal M. Al-Aamri, Syed Rehan Ahmad Zaidi, Amer A. Al-Tuwailib
  • Publication number: 20170283678
    Abstract: Disclosed is a method for modifying bentonite to allow the bentonite to be useful in drilling mud applications. The method includes the steps of: preparing bentonite local to Saudi Arabia using raw water to remove contaminants from the bentonite; grinding the bentonite to a fine powder; sieving the fine powder to be between about 50 ?m and about 150 ?m in particle size to produce a sieved fine powder; mixing the sieved fine powder with polyanionic cellulose polymer to produce a modified bentonite composition; adding the modified bentonite composition to water until a homogeneous solution of modified bentonite in water is formed; and allowing the homogeneous solution of modified bentonite in water to rest for about 16 hours to form a composition useful in drilling mud applications.
    Type: Application
    Filed: April 1, 2016
    Publication date: October 5, 2017
    Applicant: Saudi Arabian Oil Company
    Inventors: Mansour A. Al-Shafei, Akram A. Alfliow, Awad M. Al-Mofleh, Jamal M. Al-Aamri, Syed Rehan Ahmad Zaidi, Amer A. Al-Tuwailib