Patents by Inventor Jean Pierre Jules Baekelandt

Jean Pierre Jules Baekelandt has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 7727346
    Abstract: A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities?0.05 each up to a total of max. 0.15, and balance aluminium.
    Type: Grant
    Filed: April 25, 2007
    Date of Patent: June 1, 2010
    Assignees: Corus Aluminum NV, Corus Aluminum Walzprodukte GmbH
    Inventors: Job Anthonius Van Der Hoeven, Linzong Zhuang, Bruno Schepers, Peter De Smet, Jean Pierre Jules Baekelandt
  • Publication number: 20080289732
    Abstract: Method for making an aluminium-magnesium alloy in the form of a rolled product, having the composition in weight percent of: Mg 4.8-5.6, Mn 0.05-0.4, Zn 0.40-0.6, Cu 0.06-0.35, Cr 0.25 max., Fe 0.35 max., Si 0.25 max., Zr 0.12 max., Ti 0.3 max., others (each) max. 0.05, (total) max. 0.15, and balance aluminium.
    Type: Application
    Filed: July 29, 2008
    Publication date: November 27, 2008
    Applicants: CORUS ALUMINIUM NV, CORUS ALUMINIUM WALZPRODUKTE GMBH
    Inventors: Job Anthonius Van Der Hoeven, Linzhong Zhuang, Bruno Schepers, Peter De Smet, Jean Pierre Jules Baekelandt
  • Publication number: 20070187009
    Abstract: A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities?0.05 each up to a total of max. 0.15, and balance aluminium.
    Type: Application
    Filed: April 25, 2007
    Publication date: August 16, 2007
    Applicants: Aleris Aluminum Koblenz GmbH, Aleris Aluminum Duffel BVBA
    Inventors: Job Van Der Hoeven, Linzong Zhuang, Bruno Schepers, Peter De Smet, Jean Pierre Jules Baekelandt
  • Publication number: 20040261922
    Abstract: The invention relates to a wrought aluminium-magnesium alloy product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; Cr<0.25; Fe<0.35; Si<0.2; Zr<0.25; Ti<0.3; others≦0.05, each up to a total of max. 0.15, and balance aluminium.
    Type: Application
    Filed: August 27, 2004
    Publication date: December 30, 2004
    Inventors: Job Anthonius Van Der Hoeven, Linzong Zhuang, Bruno Schepers, Peter De Smet, Jean Pierre Jules Baekelandt
  • Publication number: 20040256036
    Abstract: Aluminium-magnesium alloy in the form of a rolled product or an extrusion, having the composition in weight percent:—Mg 4.5-5.6 Mn 0.05-0.4 Zn 0.40-0.8 Cu 0.06-0.35 Cr 0.25 max. Fe 0.35 max. Si 0.25 max. Zr 0.12 max. Ti 0.3 max. others (each) max. 0.05, (total) max. 0.15 balance aluminium.
    Type: Application
    Filed: August 27, 2004
    Publication date: December 23, 2004
    Inventors: Job Anthonius Van Der Hoeven, Linzhong Zhuang, Bruno Schepers, Peter De Smet, Jean Pierre Jules Baekelandt
  • Publication number: 20030145912
    Abstract: Aluminium-magnesium alloy in the form of a rolled product or an extrusion, having the following composition in weight percent: 1 Mg >3.0-4.5 Mn   0.4-1.2 Zn   0.4-1.7 Zr   0.05-0.25 Cr   0.3 max. Ti   0.2 max. V   0.2 max. Li   0.5 max. Sc   0.5 max. Fe   0.5 max. Si   0.5 max. Cu   0.15 max. Ag   0.4 max. others (each) max. 0.05 (total) max. 0.15 balance aluminium.
    Type: Application
    Filed: November 20, 2002
    Publication date: August 7, 2003
    Inventors: Alfred Johann Peter Haszler, Desikan Sampath, Jean Pierre Jules Baekelandt, Job Anthonius Van Der Hoeven