  • Publication number: 20070225517
    Abstract: Flame retardant formulations comprised of at least one bromine-containing polyol are produced by a process which comprises: A) heating a mixture formed from components comprised of (i) tetrabromophthalic anhydride, (ii) at least one aliphatic polyol, and (iii) at least one liquid straight chain aliphatic diester of a straight-chain alkane dicarboxylic acid to form an intermediate composition; and B) contacting all or a portion of the intermediate composition one or more times with (iv) at least one alkylene oxide that results in the formation of a liquid product formulation, and optionally, removing any excess alkylene oxide present; the amounts of (i), (ii), (iii), and (iv) used being proportioned to form a formulation having a bromine content of at least about 40 wt %, a viscosity at 25° C. of about 20,000 cps or less, and an acid number as determinable by aqueous sodium hydroxide titration and expressed in terms of potassium hydroxide, of less than about 1 milligram of KOH per gram of the formulation.
    Type: Application
    Filed: May 21, 2007
    Publication date: September 27, 2007
    Applicant: ALBEMARLE CORPORATION
    Inventors: Elbert Feske, Nelson Clark, Arthur Mack, Jeffrey Aplin
  • Publication number: 20070004870
    Abstract: Preparing brominated styrenic polymer by maintaining a mixture formed from (i) brominating agent, (ii) a solvent solution of styrenic polymer, and (iii) aluminum halide catalyst, at ?20 to +20° C., and terminating bromination in 20 minutes or less. New brominated anionic styrenic polymers have better melt flow and/or lower initial ?E values than the best previously-known brominated anionic styrenic polymers. Other features of such new polymers include high thermal stabilities at 320° C. and/or very low initial color values. Brominated styrenic polymers, especially brominated anionic styrenic polymers, are useful as flame retardants for thermoplastic polymers.
    Type: Application
    Filed: June 14, 2006
    Publication date: January 4, 2007
    Inventors: Charles Kolich, Jeffrey Aplin, John Balhoff
  • Publication number: 20050113495
    Abstract: Provided are new flame retardants and liquid flame retardant additive compositions of low viscosity for use in flexible polyurethane foams. The new flame retardants are the reaction product of at least one brominated aromatic diester diol with at least one alcohol-reactive agent. Preferred liquid flame retardant additive compositions are capable of minimizing visible scorching of the foam during its production. Flexible flame retardant polyurethane foams and methods for their production are also provided. The flame retardant additive compositions are formed at least from a) at least one reaction product of a brominated aromatic diester diol and an alcohol-reactive agent; b) at least one hindered amine antioxidant; and c) at least one phenolic antioxidant in which the phenolic ring is substituted by an alkanoic acid alkyl ester group in which alkanoic acid moiety has in the range of 2 to about 4 carbon atoms and the alkyl group has in the range of about 6 to about 16 carbon atoms.
    Type: Application
    Filed: November 21, 2003
    Publication date: May 26, 2005
    Inventors: Saadat Hussain, Jeffrey Aplin, William Brown, Charles Kolich, Arthur Mack
  • Publication number: 20050045857
    Abstract: A flame retardant formulation which is the combination of at least (1) at least one bromine-containing polyol flame retardant formed from the reaction of (a) tetrabromophthalic anhydride, (b) an aliphatic polyol, and (c) an epoxide, and (2) at least one aliphatic diester of an alkane dicarboxylic acid, with the proviso that the formulation has a viscosity at 25° C. of about 20,000 cps or less, and a bromine content of at least about 40 wt %. A flame retardant compound formed from A) tetrabromophthalic anhydride; B) diethylene glycol; C) at least one alpha-omega alkane diol, or at least one alpha-omega alkane diol and at least one aliphatic monool; and D) at least one alkylene oxide; with the proviso that the compound has a viscosity at 25° C. of about 60,000 cps or less, and a bromine content of at least about 43 wt %. Polymer compositions formed from (a) a polyurethane or a polyisocyanurate and (b) a formulation of the invention.
    Type: Application
    Filed: August 29, 2003
    Publication date: March 3, 2005
    Inventors: Elbert Feske, Nelson Clark, Arthur Mack, Jeffrey Aplin
  • Publication number: 20050045858
    Abstract: Flame retardant formulations comprised of at least one bromine-containing polyol are produced by a process which comprises: A) heating a mixture formed from components comprised of (i) tetrabromophthalic anhydride, (ii) at least one aliphatic polyol, and (iii) at least one liquid straight chain aliphatic diester of a straight-chain alkane dicarboxylic acid to form an intermediate composition; and B) contacting all or a portion of the intermediate composition one or more times with (iv) at least one alkylene oxide that results in the formation of a liquid product formulation, and optionally, removing any excess alkylene oxide present; the amounts of (i), (ii), (iii), and (iv) used being proportioned to form a formulation having a bromine content of at least about 40 wt %, a viscosity at 25° C. of about 20,000 cps or less, and an acid number as determinable by aqueous sodium hydroxide titration and expressed in terms of potassium hydroxide, of less than about 1 milligram of KOH per gram of the formulation.
    Type: Application
    Filed: May 20, 2004
    Publication date: March 3, 2005
    Inventors: Elbert Feske, Nelson Clark, Arthur Mack, Jeffrey Aplin