  • Patent number: 10916767
    Abstract: A method for preparing a carbon-coated ternary positive electrode material has steps of preparing a ternary positive electrode material precursor, and preparing a suspension of the ternary positive electrode material precursor. Lithium acrylate is added to the suspension of the ternary positive electrode material precursor according to the molar ratio of Li:(Ni+Co+Mn) being 1.03-1.05:1. Ammonium persulphate is added to the lithium acrylate-containing suspension of the ternary positive electrode material precursor, so that the lithium acrylate undergoes a polymerisation reaction and a suspension of a lithium polyacrylate-coated ternary positive electrode material precursor is obtained. The suspension of the lithium polyacrylate-coated ternary positive electrode material precursor is dried to obtain spherical particles. The lithium polyacrylate-coated ternary positive electrode material precursor particles are sintered to obtain a carbon-coated ternary positive electrode material.
    Type: Grant
    Filed: May 27, 2016
    Date of Patent: February 9, 2021
    Assignee: Graduate School at Shenzhen, Tsinghua University
    Inventors: Xiao-Dong Chu, Jian-Fu He, Bao-Hua Li, Yan-Bing He, Yu-Xiu Liu, Hong-Da Du, Fei-Yu Kang
  • Publication number: 20180226639
    Abstract: A method for preparing a carbon-coated ternary positive electrode material has steps of preparing a ternary positive electrode material precursor, and preparing a suspension of the ternary positive electrode material precursor. Lithium acrylate is added to the suspension of the ternary positive electrode material precursor according to the molar ratio of Li:(Ni+Co+Mn) being 1.03-1.05:1. Ammonium persulphate is added to the lithium acrylate-containing suspension of the ternary positive electrode material precursor, so that the lithium acrylate undergoes a polymerisation reaction and a suspension of a lithium polyacrylate-coated ternary positive electrode material precursor is obtained. The suspension of the lithium polyacrylate-coated ternary positive electrode material precursor is dried to obtain spherical particles. The lithium polyacrylate-coated ternary positive electrode material precursor particles are sintered to obtain a carbon-coated ternary positive electrode material.
    Type: Application
    Filed: May 27, 2016
    Publication date: August 9, 2018
    Inventors: XIAO-DONG CHU, JIAN-FU HE, BAO-HUA LI, YAN-BING HE, YU-XIU LIU, HONG-DA DU, FEI-YU KANG