  • Patent number: 9375687
    Abstract: The invention discloses an environmentally-friendly pasty discharge agent for textile printing and a method for preparing the environmentally-friendly pasty discharge agent. The environmentally-friendly pasty discharge agent for textile printing is formed by the following raw materials according to part by weight: decamethylcyclopentasiloxane: 30-60 parts; thiourea dioxide: 40-70 parts; surfactant: 1-3 parts; and glycerol: 3-6 parts. Decamethylcyclopentasiloxane is put into a ball mill, a surfactant is added into the ball mill to make the decamethylcyclopentasiloxane dispersed or dissolved uniformly and then stirred uniformly, and then thiourea dioxide is added into the ball mill and ground together for 1-3 hours. In the invention, the special liquid compound decamethylcyclopentasiloxane does not chemically react with the thiourea dioxide; in addition, it isolates the thiourea dioxide from outside water and air, thus increasing the stability of the thiourea dioxide.
    Type: Grant
    Filed: December 10, 2012
    Date of Patent: June 28, 2016
    Assignee: ZHEJIANG SCI-TECH UNIVERSITY
    Inventors: Jianzhong Shao, Lan Zhou, Yani Chen, Dongming Qi, Jinqiang Liu
  • Publication number: 20140148518
    Abstract: The invention discloses an environmentally-friendly pasty discharge agent for textile printing and a method for preparing the environmentally-friendly pasty discharge agent. The environmentally-friendly pasty discharge agent for textile printing is formed by the following raw materials according to part by weight: decamethylcyclopentasiloxane: 30-60 parts; thiourea dioxide: 40-70 parts; surfactant: 1-3 parts; and glycerol: 3-6 parts. Decamethylcyclopentasiloxane is put into a ball mill, a surfactant is added into the ball mill to make the decamethylcyclopentasiloxane dispersed or dissolved uniformly and then stirred uniformly, and then thiourea dioxide is added into the ball mill and ground together for 1-3 hours. In the invention, the special liquid compound decamethylcyclopentasiloxane does not chemically react with the thiourea dioxide; in addition, it isolates the thiourea dioxide from outside water and air, thus increasing the stability of the thiourea dioxide.
    Type: Application
    Filed: December 10, 2012
    Publication date: May 29, 2014
    Applicant: ZHEJIANG SCI-TECH UNIVERSITY
    Inventors: Jianzhong Shao, Lan Zhou, Yani Chen, Dongming Qi, Jinqiang Liu