Patents by Inventor Jorn Grossmann

Jorn Grossmann has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20140293552
    Abstract: A power semiconductor module, and method for its manufacture, comprising a first housing part having a cutout and a DC voltage load connection apparatus forming a structural unit, wherein the DC voltage load connection apparatus has first and second DC voltage load connection elements. The first DC voltage load connection element has a first leadthrough section arranged in the cutout, and the second DC voltage load connection element has a second leadthrough section arranged in the cutout forming a gap therebetween. The first and second leadthrough sections are sheathed by an elastomer, which fills the gap, is cohesively connected to the first and second leadthrough sections and seals off the first and second leadthrough sections with respect to the first housing part. The inventive power semiconductor module exhibits a high resistance to thermal cycling, and the distance between the DC voltage load connection elements can be configured to be small.
    Type: Application
    Filed: March 27, 2014
    Publication date: October 2, 2014
    Applicant: Semikron Elektronik GmbH & Co., KG
    Inventors: Ingo BOGEN, Jörn GROßMANN, Christian WALTER, Christian GÖBL
  • Publication number: 20060113009
    Abstract: A high-temperature component made of a nickel super-alloy has the following composition in wt %: 11-13% of Cr, 3-5% of W, 0.5-2.5% of Mo, 3-5% of Al, 3-5% of Ti, 3-7% of Ta, 1-5% of Re and a remainder of nickel.
    Type: Application
    Filed: July 13, 2005
    Publication date: June 1, 2006
    Inventors: Ralf Burgel, Winfried Esser, Jorn Grossmann, Wolfgang Hermann, Hael Mughrabi, Jurgen Preuhs, Florian Pyczak, Alfred Scholz, Robert Singer, Andreas Volek
  • Patent number: 7005015
    Abstract: A high-temperature component made of a nickel super-alloy has the following composition in wt %: 11–13% of Cr, 3–5% of W, 0.5–2.5% of Mo, 3–5% of Al, 3–5% of Ti, 3–7% of Ta, 1–5% of Re and a remainder formed of nickel. A corresponding component which is also provided is formed of an alloy having a composition essentially similar to that mentioned above, but with the rhenium proportion replaced with 0.1–5 wt % of ruthenium.
    Type: Grant
    Filed: January 29, 2002
    Date of Patent: February 28, 2006
    Assignee: Seimens Aktiengesellschaft
    Inventors: Ralf Bürgel, Winfried Esser, Jörn Grossmann, Wolfgang Hermann, Hael Mughrabi, Jürgen Preuhs, Florian Pyczak, Alfred Scholz, Robert Singer, Andreas Volek
  • Patent number: 6896036
    Abstract: To prevent movement of a ceramic core in a ceramic shell for the investment casting of a turbine blade, the free end of the core has one or more pins embedded therein so that the pins project into both the core and the ceramic shell which is applied over a wax layer. After removal of the wax and firing of the shell, molten metal is cast in the space left by the wax between the core and the shell. After hardening of the metal, the outwardly projecting part of the pins are removed during the machining of the surfaces of the turbine blade blank.
    Type: Grant
    Filed: August 7, 2003
    Date of Patent: May 24, 2005
    Assignee: Doncasters Precision Castings-Bochum GmbH
    Inventors: Wilfried Schneiders, Theodor Schmitte, Jörn Grossmann
  • Publication number: 20040055736
    Abstract: To prevent movement of a ceramic core in a ceramic shell for the investment casting of a turbine blade, the free end of the core has one or more pins embedded therein so that the pins project into both the core and the ceramic shell which is applied over a wax layer. After removal of the wax and firing of the shell, molten metal is cast in the space left by the wax between the core and the shell. After hardening of the metal, the outwardly projecting part of the pins are removed during the machining of the surfaces of the turbine blade blank.
    Type: Application
    Filed: August 7, 2003
    Publication date: March 25, 2004
    Applicant: DONCASTERS PRECISION CASTINGS-BOCHUM GMBH
    Inventors: Wilfried Schneiders, Theodor Schmitte, Jorn Grossmann
  • Publication number: 20020157738
    Abstract: A high-temperature component made of a nickel super-alloy has the following composition in wt %: 11-13% of Cr, 3-5% of W, 0.5-2.5% of Mo, 3-5% of Al, 3-5% of Ti, 3-7% of Ta, 1-5% of Re and a remainder formed of nickel. A corresponding component which is also provided is formed of an alloy having a composition essentially similar to that mentioned above, but with the rhenium proportion replaced with 0.1-5 wt % of ruthenium.
    Type: Application
    Filed: January 29, 2002
    Publication date: October 31, 2002
    Inventors: Ralf Burgel, Winfried Esser, Jorn Grossmann, Wolfgang Hermann, Hael Mughrabi, Jurgen Preuhs, Florian Pyczak, Alfred Scholz, Robert Singer, Andreas Volek