  • Patent number: 7569639
    Abstract: A rubber composition containing 100 parts by weight a sulfur-vulcanizable rubber (A) and 0.1 to 30 parts by weight of a vulcanization agent of a cyclic polysulfide (B) having the formula (I): wherein R is a substituted or unsubstituted C2 to C20 alkylene group, substituted or unsubstituted C2 to C20 oxyalkylene group or alkylene group having an aromatic ring, n is an integer of 1 to 20, x is a number of 2 to 6 on average.
    Type: Grant
    Filed: October 13, 2004
    Date of Patent: August 4, 2009
    Assignee: The Yokohama Rubber Co., Ltd.
    Inventors: Wonmun Choi, Tomoyuki Matsumura, Naoya Amino, Kazuhiro Takase, Daisuke Kanenari, Takeshi Hotaka, Junichirou Natori
  • Publication number: 20060094831
    Abstract: A rubber composition containing 100 parts by weight a sulfur-vulcanizable rubber (A) and 0.1 to 30 parts by weight of a vulcanization agent of a cyclic polysulfide (B) having the formula (I): wherein R is a substituted or uhsubstituted C2 to C20 alkylene group, substituted or unsubstituted C2 to C20 oxyalkylene group or alkylene group having an aromatic ring, n is an integer of 1 to 20, x is a number of 2 to 6 on average.
    Type: Application
    Filed: October 13, 2004
    Publication date: May 4, 2006
    Inventors: Wonmun Choi, Tomoyuki Matsumura, Naoya Amino, Kazuhiro Takase, Daisuke Kanenari, Takeshi Hotaka, Junichirou Natori
  • Patent number: 6984706
    Abstract: A diene rubber (A) having a weight average molecular weight (Mw) of 100,000 to 3,000,000, an Mw/number average molecular weight (Mn) ratio of 1.30 to 2.50, and an Mw/peak top molecular weight (Mp) ratio 0.70 to 1.30. A rubber composition comprising the diene rubber (A) and a diene rubber (B) having an Mw of 2,000 to 90,0000 and/or an oil extender for rubber has good processability and can give a rubber vulcanizate having high tensile strength and good abrasion resistance. The diene rubber (A) is produced by conducting a living polymerization of diene monomer in a hydrocarbon solvent; adding a polymerization stopper to a polymerization mixture at a conversion of 5 to 98% to deactivate 10 to 90% by mole of active terminals present as of the initiation of polymerization; and finally adding a polymerization stopper to completely terminate the polymerization reaction.
    Type: Grant
    Filed: March 14, 2003
    Date of Patent: January 10, 2006
    Assignee: Zeon Corporation
    Inventors: Takeshi Karato, Masaaki Komatu, Kazuhiro Takase
  • Publication number: 20050154156
    Abstract: A diene rubber (A) having a weight average molecular weight (Mw) of 100,000 to 3,000,000, an Mw/number average molecular weight (Mn) ratio of 1.30 to 2.50, and an Mw/peak top molecular weight (Mp) ratio 0.70 to 1.30. A rubber composition comprising the diene rubber (A) and a diene rubber (B) having an Mw of 2,000 to 90,0000 and/or an oil extender for rubber has good processability and can give a rubber vulcanizate having high tensile strength and good abrasion resistance. The diene rubber (A) is produced by conducting a living polymerization of diene monomer in a hydrocarbon solvent; adding a polymerization stopper to a polymerization mixture at a conversion of 5 to 98% to deactivate 10 to 90% by mole of active terminals present as of the initiation of polymerization; and finally adding a polymerization stopper to completely terminate the polymerization reaction.
    Type: Application
    Filed: March 14, 2003
    Publication date: July 14, 2005
    Applicant: ZEON CORP.
    Inventors: Takeshi Karato, Masaaki Komatu, Kazuhiro Takase