  • Publication number: 20240066639
    Abstract: An aluminum-alloy, fin material is composed of a brazing sheet containing a core material and filler material(s) disposed on both sides of the core material. The core material is an aluminum alloy containing 0.02-0.80 mass % Si, 0.02-0.80 mass % Fe, and 0.8-2.0 mass % Mn. The core material has a crystalline-aggregate structure in which: the orientation density of one or more of brass orientation, copper orientation, and S orientation is 20 times or more that or those of a randomly oriented sample; and the orientation densities of cube orientation, CR orientation, and P orientation are each 10 times or less than those of the randomly oriented sample. The filler material(s) is (are) composed of an Al—Si series alloy that contains 6.0-13.0 mass % Si and 0.02-0.80 mass % Fe. The clad percentage of filler material(s) is 6-16% of the total thickness of the brazing sheet.
    Type: Application
    Filed: January 14, 2022
    Publication date: February 29, 2024
    Inventors: Kazushige NORIKANE, Makoto ANDO
  • Patent number: 10221472
    Abstract: A structural aluminum alloy plate includes 7.0% to 12.0% by mass of Zn, 1.5% to 4.5% by mass of Mg, 1.0% to 3.0% by mass of Cu, 0.05% to 0.30% by mass of Zr, 0.005% to 0.5% by mass of Ti, 0.5% or less by mass of Si, 0.5% or less by mass of Fe, 0.3% or less by mass of Mn, 0.3% or less by mass of Cr, and the balance that includes aluminum and inevitable impurities. A method of producing the structural aluminum alloy plate is also provided.
    Type: Grant
    Filed: November 13, 2014
    Date of Patent: March 5, 2019
    Assignee: UACJ CORPORATION
    Inventors: Hidetaka Nakanishi, Kazushige Norikane, Mineo Asano
  • Publication number: 20170016102
    Abstract: A structural aluminum alloy plate includes 7.0% to 12.0% by mass of Zn, 1.5% to 4.5% by mass of Mg, 1.0% to 3.0% by mass of Cu, 0.05% to 0.30% by mass of Zr, 0.005% to 0.5% by mass of Ti, 0.5% or less by mass of Si, 0.5% or less by mass of Fe, 0.3% or less by mass of Mn, 0.3% or less by mass of Cr, and the balance that includes aluminum and inevitable impurities. A method of producing the structural aluminum alloy plate is also provided.
    Type: Application
    Filed: November 13, 2014
    Publication date: January 19, 2017