  • Publication number: 20090152383
    Abstract: A thermoplastic polymer powder which (i) consists mainly of an acrylic block copolymer comprising one or more acrylic ester polymer blocks (A) and bonded thereto at least one polymer block selected among methacrylic ester polymer blocks (B) and acrylic ester polymer blocks (C) differing in structure from the blocks (A); (ii) has a complex dynamic viscosity ?*(5) of 5.0×103 Pa·s or lower as measured under the conditions of a temperature of 250° C. and an oscillation frequency of 5 rad/sec; (iii) has a Newtonian viscosity index n represented by the equation n=log ?*(5)?log ?*(50) [wherein ?*(5) and ?*(50) indicate the complex dynamic viscosities (unit, Pa·s) as measured under the conditions of a temperature of 250° C. and oscillation frequencies of 5 and 50 rad/sec, respectively] of 0.50 or smaller; and (iv) has an average particle diameter of 1 mm or smaller. The thermoplastic polymer powder is suitable for use in molding techniques employing a powder, such as slush molding and in powder coating.
    Type: Application
    Filed: February 13, 2009
    Publication date: June 18, 2009
    Applicant: Kuraray Co., Ltd.
    Inventors: Toyoaki KURIHARA, Kenichi Hamda
  • Publication number: 20060036030
    Abstract: A thermoplastic polymer powder which (i) consists mainly of an acrylic block copolymer comprising one or more acrylic ester polymer blocks (A) and bonded thereto at least one polymer block selected among methacrylic ester polymer blocks (B) and acrylic ester polymer blocks (C) differing in structure from the blocks (A); (ii) has a complex dynamic viscosity ?*(5) of 5.0×103 Pa.s or lower as measured under the conditions of a temperature of 250° C. and an oscillation frequency of 5 rad/sec; (iii) has a Newtonian viscosity index n represented by the equation n=log ?*(5)-log ?*(50) [wherein ?*(5) and ?*(50) indicate the complex dynamic viscosities (unit, Pa.s) as measured under the conditions of a temperature of 250° C. and oscillation frequencies of 5 and 50 rad/sec, respectively] of 0.50 or smaller; and (iv) has an average particle diameter of 1 mm or smaller. The thermoplastic polymer powder is suitable for use in molding techniques employing a powder, such as slush molding and in powder coating.
    Type: Application
    Filed: October 30, 2003
    Publication date: February 16, 2006
    Applicant: Kuraray Co., Ltd.
    Inventors: Toyoaki Kurihara, Kenichi Hamda