Patents by Inventor Kiyohito Sasaki
Kiyohito Sasaki has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).
-
Patent number: 10464174Abstract: A wire includes, in terms of % by mass with respect to a total mass of the wire, as a total in a steel outer skin and a flux, 0.03 to 0.09% of C, 0.1 to 0.6% of Si, 1.3 to 2.6% of Mn, 0.01 to 0.5% of Cu, 0.05 to 0.5% of Ti, 0.002 to 0.015% of B, and 0.05% or less of Al, and further including, in the flux, 5 to 9% in terms of TiO2, 0.1 to 0.6% of in terms of SiO2, 0.02 to 0.3% in terms of Al2O3, 0.1 to 0.8% of Mg, 0.05 to 0.3% in terms of F, 0.05 to 0.3% in terms of Na and K in a fluorine compound, 0.05 to 0.2% of Na2O and K2O, and 0.1% or less in terms of ZrO2.Type: GrantFiled: November 15, 2016Date of Patent: November 5, 2019Assignee: NIPPON STEEL WELDING & ENGINEERING CO., LTD.Inventors: Kiyohito Sasaki, Rikiya Takayama, Yasuhito Totsuka
-
Publication number: 20190217423Abstract: A flux-cored wire includes by mass %: C in a skin of 0.04 to 0.08% w.r.t. a total mass of the skin, w.r.t. a total mass of the wire by a sum of the skin and flux: C: 0.05 to 0.12%, Si: 0.1 to 0.6%, Mn: 1.5 to 3.5%, B: 0.002 to 0.015%, a sum of Al2O3 conversion value of Al and Al2O3 conversion value of an Al oxide: 0.3 to 1.5%, and w.r.t. the total mass of the wire in the flux: Mg: 0.2 to 0.8%, and sums of TiO2 conversion value of a Ti oxide: 5 to 10%, SiO2 conversion value of a Si oxide: 0.2 to 0.7%, ZrO2 conversion value of a Zr oxide: 0.1 to 0.6%, F conversion value of a fluorine compound: 0.02 to 0.15%, and Na2O conversion value and a K2O conversion value of a Na compound and a K compound: 0.03 to 0.20%.Type: ApplicationFiled: January 15, 2019Publication date: July 18, 2019Applicant: NIPPON STEEL AND SUMIKIN WELDING CO., LTD.Inventors: Naoki SAKABAYASHI, Kiyohito SASAKI, Ryutaro CHIBA
-
Patent number: 10160065Abstract: A flux-cored wire for carbon dioxide gas shielded arc welding including, in terms of % by mass with respect to a total mass of the wire, 0.03 to 0.08% of C, 0.2 to 0.7% of Si, 1.4 to 3.0% of Mn, 0.01 to 0.5% of Cu, 0.8 to 3.0% of Ni, 0.05 to 0.5% of Ti, 0.002 to 0.015% of B, 0.05% or less of Al, 4 to 8% in terms of TiO2, 0.1 to 0.6% of in terms of SiO2, 0.02 to 0.3% in terms of Al2O3, 0.1 to 0.8% of Mg, 0.05 to 0.3% in terms of F, 0.05 to 0.3% in terms of Na and K in a fluorine compound, 0.05 to 0.2% of Na2O and K2O, and 0.2% or less in terms of ZrO2.Type: GrantFiled: January 13, 2016Date of Patent: December 25, 2018Assignee: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Rikiya Takayama, Kiyohito Sasaki, Yasuhito Totsuka, Masaaki Toriyabe
-
Patent number: 10112267Abstract: A wire including, in terms of % by mass with respect to a total mass of the wire, as a total in a steel outer skin and a flux, 0.03 to 0.08% of C, 0.1 to 0.6% of Si, 1.2 to 2.5% of Mn, 0.01 to 0.5% of Cu, 0.5 to 1.5% of Ni, 0.05 to 0.5% of Ti, 0.002 to 0.015% of B, and 0.05% or less of Al, and further including, in the flux, 4 to 8% in terms of TiO2, 0.1 to 0.6% of in terms of SiO2, 0.02 to 0.3% in terms of Al2O3, 0.1 to 0.8% of Mg, 0.05 to 0.3% in terms of F, 0.05 to 0.3% in terms of Na and K in a fluorine compound, 0.05 to 0.2% of Na2O and K2O, and 0.2% or less in terms of ZrO2.Type: GrantFiled: January 12, 2016Date of Patent: October 30, 2018Assignee: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Rikiya Takayama, Kiyohito Sasaki, Yasuhito Totsuka, Masaaki Toriyabe
-
Publication number: 20180272477Abstract: A flux-cored wire for gas-shielded arc welding, including, in terms of mass % relative to a total mass of the wire, in the total of the steel outer sheath and the flux, C: 0.03 to 0.08%, Si: 0.1 to 0.6%, Mn: 1.5 to 2.8%, Cu: 0.01 to 0.5%, Ni: 0.35 to 0.98%, Ti: 0.05 to 0.25%, and B: 0.002 to 0.015%, Al: 0.05% or less, and including, in the flux, TiO2 conversion value: 3 to 8%, Al2O3 conversion value: 0.1 to 0.6%, SiO2 conversion value: 0.2 to 1.0%, ZrO2 conversion value: 0.20 to 0.65%, Mg: 0.2 to 0.8%, F conversion value: 0.05 to 0.25%, Na conversion value: 0.02 to 0.10%, and K conversion value: 0.05 to 0.20%.Type: ApplicationFiled: March 16, 2018Publication date: September 27, 2018Applicant: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Kiyohito SASAKI, Naoki SAKABAYASHI, Ryutaro CHIBA
-
Publication number: 20180056454Abstract: A flux-cored wire for gas shielded arc welding includes C: 0.03 to 0.09%, Si: 0.1 to 0.6%, Mn: 1.3 to 3.0%, Ti: 0.05 to 0.50%, B: 0.002 to 0.015%, and Al2O3 converted value: 0.4 to 1.0%, as the total content in the steel sheath and the flux in mass % relative to the total mass of the wire; and TiO2 converted value: 5.0 to 9.0%, SiO2 converted value: 0.2 to 0.7%, ZrO2 converted value: 0.1 to 0.6%, Mg: 0.2 to 0.8%, total of F converted value: 0.02 to 0.20%, and total of Na2O converted value and K2O converted value: 0.03 to 0.20%; as a content in the flux; in which a content of C in the steel sheath is 0.03% or less in mass % relative to the total mass of the steel sheath.Type: ApplicationFiled: July 5, 2017Publication date: March 1, 2018Applicant: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Yuki KAYAMORI, Kiyohito SASAKI, Yasuhito TOTSUKA, Naoki SAKABAYASHI
-
Publication number: 20170144257Abstract: A wire includes, in terms of % by mass with respect to a total mass of the wire, as a total in a steel outer skin and a flux, 0.03 to 0.09% of C, 0.1 to 0.6% of Si, 1.3 to 2.6% of Mn, 0.01 to 0.5% of Cu, 0.05 to 0.5% of Ti, 0.002 to 0.015% of B, and 0.05% or less of Al, and further including, in the flux, 5 to 9% in terms of TiO2, 0.1 to 0.6% of in terms of SiO2, 0.02 to 0.3% in terms of Al2O3, 0.1 to 0.8% of Mg, 0.05 to 0.3% in terms of F, 0.05 to 0.3% in terms of Na and K in a fluorine compound, 0.05 to 0.2% of Na2O and K2O, and 0.1% or less in terms of ZrO2.Type: ApplicationFiled: November 15, 2016Publication date: May 25, 2017Applicant: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Kiyohito SASAKI, Rikiya TAKAYAMA, Yasuhito TOTSUKA
-
Publication number: 20170129056Abstract: A flux-cored wire for carbon dioxide gas shielded arc welding includes, in terms of % by mass with respect to a total mass of the wire, 0.03 to 0.08% of C, 0.2 to 0.6% of Si, 1.2 to 2.8% of Mn, 0.01 to 0.5% of Cu, 0.2 to 0.7% of Ni, 0.1 to 0.6% of Ti, 0.005 to 0.020% of B, 0.05% or less of Al, 4.0 to 8.0% in terms of TiO2, 0.1 to 0.6% of in terms of SiO2, 0.02 to 0.3% in terms of Al2O3, 0.1 to 0.8% of Mg, 0.05 to 0.3% in terms of F, 0.05 to 0.3% in terms of Na and K in a fluorine compound, 0.05 to 0.2% of Na2O and K2O, and 0.2% or less in terms of ZrO2.Type: ApplicationFiled: October 20, 2016Publication date: May 11, 2017Applicant: NIPPON STEEL & SUMIKIN WELDING CO., LTD.Inventors: Rikiya TAKAYAMA, Kiyohito SASAKI, Yasuhito TOTSUKA, Masaaki TORIYABE
-
Patent number: 9211613Abstract: A flux-cored wire for gas shielded welding use which can reduce the oxygen of weld metal to obtain a weld joint which is excellent in toughness and which enables all-position welding by direct current reverse polarity, wherein the wire contains, by mass % with respect to the wire total mass, CaO: 0.2 to 7.0%, one or more of MgF2, CaF2, SrF2, and BaF2 in a total of 1.0% or more (total of fluorides and CaO being 3.0 to 12.0%), one or more of Si, Al (less than 0.3%), Ti, Mg, Zr, Ca, Ce, and La in a total of 0.2 to 2.0%, and one or more oxides of Si, Mn, Al, Ti, B, and Zr in a total of 0.2 to 3.0%, ?=C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+Nb/10+5B is 0.15 to 0.40%, P and S in a total of 0.040% or less, a balance of Fe, an arc stabilizer, unavoidable impurities, and a content of iron powder in the flux of 5.0% or less.Type: GrantFiled: December 14, 2010Date of Patent: December 15, 2015Assignee: NIPPON STEEL & SUMITOMO METAL CORPORATIONInventors: Kazuhiro Kojima, Ryuichi Shimura, Kiyohito Sasaki
-
Publication number: 20120241433Abstract: A flux-cored wire for gas shielded welding use which can reduce the oxygen of weld metal to obtain a weld joint which is excellent in toughness and which enables all-position welding by direct current reverse polarity, wherein the wire contains, by mass % with respect to the wire total mass, CaO: 0.2 to 7.0%, one or more of MgF2, CaF2, SrF2, and BaF2 in a total of 1.0% or more (total of fluorides and CaO being 3.0 to 12.0%), one or more of Si, Al (less than 0.3%), Ti, Mg, Zr, Ca, Ce, and La in a total of 0.2 to 2.0%, and one or more oxides of Si, Mn, Al, Ti, B, and Zr in a total of 0.2 to 3.0%, ?=C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+Nb/10+5B is 0.15 to 0.40%, P and S in a total of 0.040% or less, a balance of Fe, an arc stabilizer, unavoidable impurities, and a content of iron powder in the flux of 5.0% or less.Type: ApplicationFiled: December 14, 2010Publication date: September 27, 2012Inventors: Kazuhiro Kojima, Ryuichi Shimura, Kiyohito Sasaki