Patents by Inventor Kuang-Hung Tseng

Kuang-Hung Tseng has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20120223068
    Abstract: A local resistance heating device with a controlled atmosphere, which includes two end members and a mid member, is provided. The two end members are respectively connected with an anode pole and a cathode pole, each end member has an air channel, the air channel of one of the end members is adapted to connect with an output terminal of a gas supplier, and the air channel of the other one of the end members is adapted to connect with a sucking terminal of the gas supplier. The mid member is arranged between the two end members, wherein the two end members and the mid member jointly define a heating room communicating with the air channels of the two end members.
    Type: Application
    Filed: April 28, 2011
    Publication date: September 6, 2012
    Inventors: Kuang-Hung Tseng, Jie-Meng Huang
  • Patent number: 7896979
    Abstract: An activating flux for welding stainless steel includes: from 25 to 40 weight percent of titanium dioxide (TiO2); from 25 to 30 weight percent of chromium oxide (Cr2O3); from 10 to 30 weight percent of silicon dioxide (SiO2); from 10 to 15 weight percent of molybdenum disulphide (MoS2); and from 5 to 15 weight percent of molybdenum trioxide (MoO3), which are active additive materials. A welding rod or wire includes a welding material and an activating flux. The activating flux layer is provided on or in the welding rod or wire and is formed as an outer layer or a core portion of the welding rod or wire.
    Type: Grant
    Filed: July 2, 2007
    Date of Patent: March 1, 2011
    Assignee: National Pingtung University of Science & Technology
    Inventors: Ping-Chung Tseng, Kuang-Hung Tseng
  • Publication number: 20100288397
    Abstract: A welding flux for stainless steel including 30-55 wt % of silicon dioxide, 20-40 wt % of titanium dioxide, 10-20 wt % of chromium oxide, 5-20 wt % of molybdenum oxide, 5-10 wt % of molybdenum sulfide, and 5-10 wt % of halide.
    Type: Application
    Filed: May 13, 2010
    Publication date: November 18, 2010
    Inventor: Kuang-Hung Tseng
  • Publication number: 20080029185
    Abstract: An activating flux for welding stainless steel includes: from 25 to 40 weight percent of titanium dioxide (TiO2); from 25 to 30 weight percent of chromium oxide (Cr2O3); from 10 to 30 weight percent of silicon dioxide (SiO2); from 10 to 15 weight percent of molybdenum disulphide (MoS2); and from 5 to 15 weight percent of molybdenum trioxide (MoO3) which are of active additive materials. A welding rod or wire includes a welding material and an activating flux. The activating flux layer is provided on or in the welding rod or wire, and is formed as an outer layer or a core portion of the welding rod or wire.
    Type: Application
    Filed: July 2, 2007
    Publication date: February 7, 2008
    Inventors: Ping-Chung Tseng, Kuang-Hung Tseng