  • Patent number: 10351424
    Abstract: The present invention provides a Ni—Zr oxide catalyst and a process for the preparation of the catalyst. The invention further provides use of the catalyst for the production of synthesis gas (a mixture of CO and H2) by Tri-reforming of methane. The process provides a direct single step selective vapor phase partial oxidation of methane to synthesis gas over Ni—ZrO2 catalyst between temperature range of 600° C. to 800° C. at atmospheric pressure. The process provides a methane conversion of 1-99% with H2 to CO mole ratio of 1.6 to 2.2.
    Type: Grant
    Filed: March 30, 2016
    Date of Patent: July 16, 2019
    Assignee: COUNCIL OF SCIENTIFIC & INDUSTRIAL RESEARCH
    Inventors: Rajaram Bal, Rajib Kumar Singha, Ankur Bordoloi, Chandrashekar Pendem, Laxmi narayan Sivakumar Konathala
  • Patent number: 9889434
    Abstract: The present invention provides a process and catalyst for the autothermal and dry reforming of methane to produce syngas. The process provides a direct single step gas phase reforming of methane or natural gas to syngas over Ni—Pt supported nanocrystalline ZrO2. The process provides methane conversion of 54-99% with H2/CO ratio of 1.14 to 1.42 (mol %) in the temperature range of 250 to 750 800° C. at atmospheric pressure.
    Type: Grant
    Filed: August 10, 2016
    Date of Patent: February 13, 2018
    Assignee: COUNCIL OF SCIENTIFIC & INDUSTRIAL RESEARCH
    Inventors: Rajaram Bal, Bipul Sarkar, Reena Goyal, Ankur Bordoloi, Chandrashekar Pendem, Laxmi Narayan Sivakumar Konathala
  • Publication number: 20170043324
    Abstract: The present invention provides a process and catalyst for the autothermal and dry reforming of methane to produce syngas. The process provides a direct single step gas phase reforming of methane or natural gas to syngas over Ni—Pt supported nanocrystalline ZrO2. The process provides methane conversion of 54-99% with H2/CO ratio of 1.14 to 1.42 (mol %) in the temperature range of 250 to 750 800° C. at atmospheric pressure.
    Type: Application
    Filed: August 10, 2016
    Publication date: February 16, 2017
    Inventors: Rajaram Bal, Bipul Sarkar, Reena Goyal, Ankur Bordoloi, Chandrashekar Pendem, Laxmi Narayan Sivakumar Konathala
  • Patent number: 9468914
    Abstract: The present invention provides an improved process for the preparation of phosphorous containing mesoporous alumina catalyst for selective dehydration of methanol to dimethyl ether. The process provides a single step selective vapor phase dehydration of methanol to produce dimethyl ether over phosphorous containing mesoporous alumina (P/Al2O3) catalyst at a temperature in the range of 150-350° C. The process provides methanol conversion of 45-100% with a selectivity of the DME up to 100%.
    Type: Grant
    Filed: February 27, 2015
    Date of Patent: October 18, 2016
    Assignee: COUNCIL OF SCIENTIFIC & INDUSTRIAL RESEARCH
    Inventors: Ankur Bordoloi, Reena Goyal, Subhasis Das, Rajib Kumar Singha, Chandrashekar Pendem, Laxmi Narayan Sivakumar Konathala, Rajaram Bal, Sandeep Saran, Madhukar Onkarnath Garg
  • Publication number: 20160289073
    Abstract: The present invention provides a Ni—Zr oxide catalyst and a process for the preparation of the catalyst. The invention further provides use of the catalyst for the production of synthesis gas (a mixture of CO and H2) by Tri-reforming of methane. The process provides a direct single step selective vapor phase partial oxidation of methane to synthesis gas over Ni—ZrO2 catalyst between temperature range of 600° C. to 800° C. at atmospheric pressure. The process provides a methane conversion of 1-99% with H2 to CO mole ratio of 1.6 to 2.2.
    Type: Application
    Filed: March 30, 2016
    Publication date: October 6, 2016
    Applicant: COUNCIL OF SCIENTIFIC & INDUSTRIAL RESEARCH
    Inventors: Rajaram Bal, Rajib Kumar Singha, Ankur Bordoloi, Chandrashekar Pendem, Laxmi narayan Sivakumar Konathala
  • Publication number: 20150336086
    Abstract: The present invention provides an improved process for the preparation of phosphorous containing mesoporous alumina catalyst for selective dehydration of methanol to dimethyl ether. The process provides a single step selective vapour phase dehydration of methanol to produce dimethyl ether over phosphorous containing mesoporous alumina (P/Al2O3) catalyst at a temperature in the range of 150-350° C. The process provides methanol conversion of 45-100% with a selectivity of the DME up to 100%.
    Type: Application
    Filed: February 27, 2015
    Publication date: November 26, 2015
    Inventors: Ankur BORDOLOI, Reena GOYAL, Subhasis DAS, Rajib Kumar SINGHA, Chandrashekar PENDEM, Laxmi Narayan Sivakumar KONATHALA, Rajaram BAL, Sandeep SARAN, Madhukar Onkarnath GARG