Patents by Inventor Lianne Rachow

Lianne Rachow has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9783712
    Abstract: A hot melt adhesive for use on porous substrates, wherein the hot melt adhesive has about 10% to about 70% by weight of a polypropylene homopolymer having a DSC melting point of less than 100° C.; about 10% to about 60% of a first tackifying resin having a Ring & Ball Softening Point of about 95° C. to about 140° C.; about 0% to about 65% of a second tackifying resin that is different than the first tackifying resin; about 5% to about 50% of a plasticizer; about 1% to about 40% by weight of a secondary polymer which is either a semi crystalline polymer or wax with an enthalpy of fusion of greater than 30 Joules/gram; about 0.1% to about 5% of a stabilizer or antioxidant; wherein the components total 100% by weight of the composition, and the viscosity of the composition is equal to or less than about 20,000 centipoise (cP) at 163° C. (325° F.).
    Type: Grant
    Filed: April 21, 2016
    Date of Patent: October 10, 2017
    Assignee: Bostik, Inc.
    Inventors: Richard Hamann, Lianne Rachow
  • Publication number: 20160230055
    Abstract: A hot melt adhesive for use on porous substrates, wherein the hot melt adhesive has about 10% to about 70% by weight of a polypropylene homopolymer having a DSC melting point of less than 100° C.; about 10% to about 60% of a first tackifying resin having a Ring & Ball Softening Point of about 95° C. to about 140° C.; about 0% to about 65% of a second tackifying resin that is different than the first tackifying resin; about 5% to about 50% of a plasticizer; about 1% to about 40% by weight of a secondary polymer which is either a semi crystalline polymer or wax with an enthalpy of fusion of greater than 30 Joules/gram; about 0.1% to about 5% of a stabilizer or antioxidant; wherein the components total 100% by weight of the composition, and the viscosity of the composition is equal to or less than about 20,000 centipoise (cP) at 163° C. (325° F.).
    Type: Application
    Filed: April 21, 2016
    Publication date: August 11, 2016
    Inventors: Richard Hamann, Lianne Rachow
  • Patent number: 9334431
    Abstract: A hot melt adhesive for use on porous substrates, wherein the hot melt adhesive has a) about 10% to about 70% by weight of a polypropylene homopolymer having a DSC melting point of less than 100° C.; b) about 10% to about 60% of a first tackifying resin having a Ring & Ball Softening Point of about 95° C. to about 140° C.; c) about 0% to about 65% of a second tackifying resin that is different than the first tackifying resin; d) about 5% to about 50% of a plasticizer; e) about 1% to about 40% by weight of a secondary polymer which is either a semi-crystalline polymer or wax with an enthalpy of fusion of greater than 30 Joules/gram; f) about 0.1% to about 5% of a stabilizer or antioxidant; wherein the components total 100% by weight of the composition, and the viscosity of the composition is equal to or less than about 20,000 centipoise (cP) at 163° C. (325° F.).
    Type: Grant
    Filed: May 21, 2014
    Date of Patent: May 10, 2016
    Assignee: BOSTIK, INC.
    Inventors: Richard Hamann, Lianne Rachow
  • Publication number: 20140350155
    Abstract: A hot melt adhesive for use on porous substrates, wherein the hot melt adhesive has a) about 10% to about 70% by weight of a polypropylene homopolymer having a DSC melting point of less than 100° C.; b) about 10% to about 60% of a first tackifying resin having a Ring & Ball Softening Point of about 95° C. to about 140° C.; c) about 0% to about 65% of a second tackifying resin that is different than the first tackifying resin; d) about 5% to about 50% of a plasticizer; e) about 1% to about 40% by weight of a secondary polymer which is either a semi-crystalline polymer or wax with an enthalpy of fusion of greater than 30 Joules/gram; f) about 0.1% to about 5% of a stabilizer or antioxidant; wherein the components total 100% by weight of the composition, and the viscosity of the composition is equal to or less than about 20,000 centipoise (cP) at 163° C. (325° F.).
    Type: Application
    Filed: May 21, 2014
    Publication date: November 27, 2014
    Applicant: Bostik, Inc.
    Inventors: Richard Hamann, Lianne Rachow