Patents by Inventor Linhui WAN

Linhui WAN has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9902005
    Abstract: A low-boron-oxygen cutting line for one-way wire winding and a manufacturing method are provided. A core material comprises 55-65 wt % of copper, 0.001-0.03 wt % of boron, 0.05-1.0 wt % of other elements which are at least two of titanium, iron, silicon, nickel, manganese, aluminum, tin, phosphorus and rare earth, less than 0.5 wt % of inevitable impurity elements, and an allowance of zinc; and a surface comprises 35.0-45.0 wt % of copper, 0.001-3.0 wt % of oxygen, 0.0005-0.5 wt % of other elements, at least two of which are titanium, iron, silicon, nickel, manganese, aluminum, tin, phosphorus and rare earth, less than 0.5 wt % of inevitable impurity elements, and an allowance of zinc. The cutting line has improved mechanical properties and strengthened discharge properties, and can cut irregularly shaped materials or those hollowed in the middle.
    Type: Grant
    Filed: June 8, 2015
    Date of Patent: February 27, 2018
    Assignee: NINGBO BODE HIGHTECH CO., LTD.
    Inventors: Xianqi Meng, Linhui Wan, Huogen Lin, Fanglin Guo, Xiaojun Chen
  • Patent number: 9855617
    Abstract: The invention discloses a high-precision zinc-based alloy electrode wire, the external shell thereof consisting of: Zn: 70.5-95%; Cu: 2.5-27%; X: 0.02-4.0%; Y: 0.002-0.4%, and unavoidable impurities; where, X refers to any two kinds of metals selected from Ni, Ag, Cr, Si and Zr, and the weight percentage of each of these two kinds of metals is 0.01-2.0%; and Y refers to any two kinds of metals selected from Ti, Al, Co, B, and P, and the weight percentage of each of these two kinds of metals is 0.001-0.2%; the ?-phase in a metallurgical structure of the external shell is above 80 wt %. The invention also provides a method for manufacturing the electrode wire, which has high surface smoothness of the cut metal workpieces to improve the cutting precision. The method has simple process, high maneuverability, less steps, so as to facilitate large-scale and automated production.
    Type: Grant
    Filed: April 21, 2015
    Date of Patent: January 2, 2018
    Assignee: Ningbo Powerway Materialise Co., Ltd.
    Inventors: Zhining Liang, Fanglin Guo, Linhui Wan, Tong Wu
  • Publication number: 20160368070
    Abstract: The invention discloses a high-precision zinc-based alloy electrode wire, the external shell thereof consisting of: Zn: 70.5-95%; Cu: 2.5-27%; X: 0.02-4.0%; Y: 0.002-0.4%, and unavoidable impurities; where, X refers to any two kinds of metals selected from Ni, Ag, Cr, Si and Zr, and the weight percentage of each of these two kinds of metals is 0.01-2.0%; and Y refers to any two kinds of metals selected from Ti, Al, Co, B, and P, and the weight percentage of each of these two kinds of metals is 0.001-0.2%; the ?-phase in a metallurgical structure of the external shell is above 80 wt %. The invention also provides a method for manufacturing the electrode wire, which has high surface smoothness of the cut metal workpieces to improve the cutting precision. The method has simple process, high maneuverability, less steps, so as to facilitate large-scale and automated production.
    Type: Application
    Filed: April 21, 2015
    Publication date: December 22, 2016
    Inventors: Zhining Liang, Fanglin Guo, Linhui Wan, Tong Wu
  • Publication number: 20160221095
    Abstract: A low-boron-oxygen cutting line for one-way wire winding and a manufacturing method are provided. A core material comprises 55-65 wt % of copper, 0.001-0.03 wt % of boron, 0.05-1.0 wt % of other elements which are at least two of titanium, iron, silicon, nickel, manganese, aluminum, tin, phosphorus and rare earth, less than 0.5 wt % of inevitable impurity elements, and an allowance of zinc; and a surface comprises 35.0-45.0 wt % of copper, 0.001-3.0 wt % of oxygen, 0.0005-0.5 wt % of other elements, at least two of which are titanium, iron, silicon, nickel, manganese, aluminum, tin, phosphorus and rare earth, less than 0.5 wt % of inevitable impurity elements, and an allowance of zinc. The cutting line has improved mechanical properties and strengthened discharge properties, and can cut irregularly shaped materials or those hollowed in the middle.
    Type: Application
    Filed: June 8, 2015
    Publication date: August 4, 2016
    Applicant: NINGBO POWERWAY MATERIALISE CO.,LTD.
    Inventors: Xianqi MENG, Linhui WAN, Huogen LIN, Fanglin GUO, Xiaojun CHEN