  • Patent number: 7638567
    Abstract: In various embodiments, the present inventions provide a rubber composite having an abrasion resistance better than about 125 mm3 under DIN 53516 and comprising a natural rubber, between about 15 to about 25 parts per hundred rubber (PHR) of a butadiene, between about 20 to about 40 PHR of a silica; and between about 0.4 to about 4 PHR of an organosilane polysulfur cross-linking agent. Also provided in various embodiments are multiply rubber materials having a first ply of the above composite and a second thinner ply of a styrene-butadiene rubber.
    Type: Grant
    Filed: January 26, 2009
    Date of Patent: December 29, 2009
    Assignee: American Biltrite (Canada) Ltd.
    Inventor: Luc-Lin Lemelin
  • Publication number: 20090133991
    Abstract: In various embodiments, the present inventions provide a rubber composite having an abrasion resistance better than about 125 mm3 under DIN 53516 and comprising a natural rubber, between about 15 to about 25 parts per hundred rubber (PHR) of a butadiene, between about 20 to about 40 PHR of a silica; and between about 0.4 to about 4 PHR of an organosilane polysulfur cross-linking agent. Also provided in various embodiments are multiply rubber materials having a first ply of the above composite and a second thinner ply of a styrene-butadiene rubber.
    Type: Application
    Filed: January 26, 2009
    Publication date: May 28, 2009
    Applicant: AMERICAN BILTRITE, INC.
    Inventor: Luc-Lin LEMELIN
  • Publication number: 20070244235
    Abstract: In various embodiments, the present inventions provide a rubber composite having an abrasion resistance better than about 125 mm3 under DIN 53516 and comprising a natural rubber, between about 15 to about 25 parts per hundred rubber (PHR) of a butadiene, between about 20 to about 40 PHR of a silica; and between about 0.4 to about 4 PHR of an organosilane polysulfur cross-linking agent. Also provided in various embodiments are multiply rubber materials having a first ply of the above composite and a second thinner ply of a styrene-butadiene rubber.
    Type: Application
    Filed: November 13, 2006
    Publication date: October 18, 2007
    Applicant: American Biltrite (Canada) Ltd.
    Inventor: Luc-Lin Lemelin