Patents by Inventor Ma WEIZENG

Ma WEIZENG has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 10730149
    Abstract: Brazing sheet having a core layer made of a first aluminium alloy, attached to one side of said core layer a sacrificial cladding made of a second aluminium alloy, and attached to the other side of said core layer a braze cladding made of a third aluminium alloy. The first aluminium alloy consists of: Si ?0.6 wt %; Fe ?0.7 wt %; Cu 0.4-0.9 wt %; Mn 1.0-1.6 wt %; Mg ?0.2 wt %; Cr 0.05-0.15 wt %; Zr 0.05-0.15 wt %; Ti 0.05-0.15 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %; the second aluminium alloy consists of: Si 0.65-1.0 wt %; Fe ?0.4 wt %; Cu ?0.05 wt %; Mn 1.4-1.8 wt %; Zn 1.5-4.0 wt %; Zr 0.05-0.20 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %. The third aluminium alloy has a melting point lower than said first and second aluminium alloys.
    Type: Grant
    Filed: November 9, 2016
    Date of Patent: August 4, 2020
    Assignee: Gränges AB
    Inventors: Sampath Desikan, Ma Weizeng
  • Publication number: 20180333809
    Abstract: Brazing sheet having a core layer made of a first aluminium alloy, attached to one side of said core layer a sacrificial cladding made of a second aluminium alloy, and attached to the other side of said core layer a braze cladding made of a third aluminium alloy. The first aluminium alloy consists of: Si ?0.6 wt %; Fe ?0.7 wt %; Cu 0.4-0.9 wt %; Mn 1.0-1.6 wt %; Mg ?0.2 wt %; Cr 0.05-0.15 wt %; Zr 0.05-0.15 wt %; Ti 0.05-0.15 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %; the second aluminium alloy consists of: Si 0.65-1.0 wt %; Fe ?0.4 wt %; Cu ?0.05 wt %; Mn 1.4-1.8 wt %; Zn 1.5-4.0 wt %; Zr 0.05-0.20 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %. The third aluminium alloy has a melting point lower than said first and second aluminium alloys.
    Type: Application
    Filed: November 9, 2016
    Publication date: November 22, 2018
    Applicant: GRÄNGES AB
    Inventors: Sampath DESIKAN, Ma WEIZENG
  • Publication number: 20180326540
    Abstract: Brazing sheet having a core layer made of a first aluminium alloy, attached to one side of said core layer a sacrificial cladding made of a second aluminium alloy, and attached to the other side of said core layer a braze cladding made of a third aluminium alloy. The first aluminium alloy consists of: Si 0.2-1.0 wt %; Fe 0.15-0.9 wt %; Cu 0.2-0.9 wt %; Mn 1.0-1.6 wt %; Mg ?0.3 wt %; Cr 0.05-0.15 wt %; Zr 0.05-0.25 wt %; Ti 0.05-0.25 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %; the second aluminium alloy consists of: Si 0.45-1.0 wt %; Fe ?0.4 wt %; Cu ?0.05 wt %; Mn 1.2-1.8 wt %; Ti ?0.10 wt %, Zn 1.3-5.5 wt %; Zr 0.05-0.20 wt %; other elements ?0.05 wt % each and ?0.2 wt % total; Al balance up to 100 wt %. Third aluminium alloy has a melting point lower than said first and second aluminium alloys.
    Type: Application
    Filed: November 9, 2016
    Publication date: November 15, 2018
    Applicant: GRÄNGES AB
    Inventors: Sampath DESIKAN, Ma WEIZENG