  • Patent number: 11135569
    Abstract: The subject matter of the invention is a method for producing composites, comprising mixed oxides of aluminum oxide and cerium/zirconium, hereinafter referred to briefly as Al/Ce/Zr oxide composite(s), using boehmite and soluble cerium/zirconium salts. Al/Ce/Zr oxide composites produced in this way have an increased thermal stability.
    Type: Grant
    Filed: January 29, 2018
    Date of Patent: October 5, 2021
    Assignees: TREIBACHER INDUSTRIE AG, SASOL GERMANY GMBH
    Inventors: Karl Schermanz, Amod Sagar, Marcos Schöneborn, Reiner Glöckler, Kai Dallman, Frank Alber, Sonke Rolfs
  • Publication number: 20180147559
    Abstract: A process for the preparation of a calcined mixed oxide comprising Al-, Ce- and Zr-oxides, comprising the steps of providing an aqueous slurry comprising hydroxides of cerium and zirconium, contacting the hydroxides of cerium and zirconium with an alumina precursor to obtain an aqueous suspension of solids, isolating the solids from the aqueous suspension and drying to obtain a solid composition, calcining the solid composition of step (c) at a temperature from 450° C. to 1200° C. for at least 1 hour to obtain a calcined mixed oxide.
    Type: Application
    Filed: January 29, 2018
    Publication date: May 31, 2018
    Inventors: Karl Schermanz, Amod Sagar, Marcos Schöneborn, Reiner Glöckler, Kai Dallman, Frank Alber, Sonke Rolfs
  • Patent number: 9889428
    Abstract: A process for the preparation of a calcined mixed oxide comprising Al-, Ce- and Zr-oxides, comprising the steps of providing an aqueous slurry comprising hydroxides of cerium and zirconium, contacting the hydroxides of cerium and zirconium with an alumina precursor to obtain an aqueous suspension of solids, isolating the solids from the aqueous suspension and drying to obtain a solid composition, calcining the solid composition of step (c) at a temperature from 450° C. to 1200° C. for at least 1 hour to obtain a calcined mixed oxide.
    Type: Grant
    Filed: July 13, 2012
    Date of Patent: February 13, 2018
    Assignees: TREIBACHER INDUSTRIE AG, SASOL GERMANY GMBH
    Inventors: Karl Schermanz, Amod Sagar, Marcos Schöneborn, Reiner Glöckler, Kai Dallmann, Frank Alber, Sönke Rolfs
  • Publication number: 20140221200
    Abstract: The subject matter of the invention is a method for producing composites comprising aluminum oxide and cerium/zirconium mixed oxides, hereinafter referred to briefly as Al/Ce/Zr oxide composite(s) using boehmite and soluble cerium/zirconium salts. Al/Ce/Zr oxide composites produced in this way have an increased thermal stability.
    Type: Application
    Filed: July 13, 2012
    Publication date: August 7, 2014
    Inventors: Marcos Schöneborn, Reiner Glöckler, Anja Paeger
  • Publication number: 20130017947
    Abstract: A process for the preparation of a calcined mixed oxide comprising Al-, Ce- and Zr-oxides, comprising the steps of providing an aqueous slurry comprising hydroxides of cerium and zirconium, contacting the hydroxides of cerium and zirconium with an alumina precursor to obtain an aqueous suspension of solids, isolating the solids from the aqueous suspension and drying to obtain a solid composition, calcining the solid composition of step (c) at a temperature from 450° C. to 1200° C. for at least 1 hour to obtain a calcined mixed oxide.
    Type: Application
    Filed: July 13, 2012
    Publication date: January 17, 2013
    Applicants: Sasol Germany GmbH, Treibacher Industries AG
    Inventors: Karl Schermanz, Amod Sagar, Marcos Schöneborn, Reiner Glöckler, Kai Dallmann, Frank Alber, Sönke Rolfs