  • Patent number: 11198743
    Abstract: A process for the continuous synthesis of a modified diene elastomer comprising at least one silicon atom directly connected to the elastomer chain is provided. The process comprises polymerization by n reactors r1 to rn, considered to be continuous stirred-tank reactors equipped with an internal stirring system and arranged in series, n varying from 2 to 15. The reactor r1 is fed by an input solution comprising a solvent, one or more monomer(s), an anionic polymerization initiator chosen from lithium amides and a polar agent. The temperature of each reactor varies from 20° C. to 150° C. and is greater than or equal to the temperature of the reactor which immediately precedes it. The living diene elastomer obtained exhibits a polydispersity index varying from 1.1 to 1.7. The process further comprises modification of the living diene elastomer obtained in the preceding stage by a functionalization, coupling or star-branching agent.
    Type: Grant
    Filed: December 20, 2017
    Date of Patent: December 14, 2021
    Assignee: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Marie-Hélène Dessendier, Charlotte Dire, Claire Fauvarque-Nuytten
  • Patent number: 11059914
    Abstract: A process for the continuous synthesis of a diene elastomer is provided. The synthesis is conducted by means of n reactors r1 to rn, considered to be continuous stirred-tank reactors, which are equipped with an internal stirring system. The reactors are arranged in series, n varying from 2 to 15, preferably from 2 to 9. The reactor r1 is fed by an input solution comprising a solvent, one or more monomer(s), an anionic polymerization initiator chosen from lithium amides and a polar agent. The conversion by weight C1 in the first reactor is less than 70%, and the total conversion by weight Cn at the outlet of the reactor rn is greater than or equal to 70%.
    Type: Grant
    Filed: December 20, 2017
    Date of Patent: July 13, 2021
    Assignee: COMPAGNIE GENERALE DES ETABLISSMENTS MICHELIN
    Inventors: Charlotte Dire, Marie-Hélène Dessendier
  • Patent number: 10562985
    Abstract: A modified diene elastomer is provided. The elastomer comprises: at least 70% by weight, with respect to the total weight of the modified diene elastomer, of a linear diene elastomer functionalized predominantly in the middle of the chain by an alkoxysilane group, optionally partially or completely hydrolysed to give silanol, the alkoxysilane group optionally bearing another functional group capable of interacting with a reinforcing filler, the alkoxysilane group bonded to the two branches of the diene elastomer via the silicon atom, the functionalized diene elastomer exhibiting a polydispersity index before fractionalization of less than or equal to 1.6; and more than 0 and up to 30% by weight, with respect to the total weight of the modified diene elastomer, of a star-branched diene elastomer exhibiting a polydispersity index before star-branching of less than or equal to 1.6, the Mooney viscosity of the modified diene elastomer varying from 30 to 80.
    Type: Grant
    Filed: July 1, 2016
    Date of Patent: February 18, 2020
    Assignee: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Marie-Hélène Dessendier, Charlotte Dire, Margarita Dorato, Jean Marc Marechal, Florent Vaultier
  • Publication number: 20190352432
    Abstract: A process for the continuous synthesis of a diene elastomer is provided. The synthesis is conducted by means of n reactors r1 to rn, considered to be continuous stirred-tank reactors, which are equipped with an internal stirring system. The reactors are arranged in series, n varying from 2 to 15, preferably from 2 to 9. The reactor r1 is fed by an input solution comprising a solvent, one or more monomer(s), an anionic polymerization initiator chosen from lithium amides and a polar agent. The conversion by weight C1 in the first reactor is less than 70%, and the total conversion by weight Cn at the outlet of the reactor rn is greater than or equal to 70%.
    Type: Application
    Filed: December 20, 2017
    Publication date: November 21, 2019
    Applicant: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Charlotte DIRE, Marie-Hélène DESSENDIER
  • Publication number: 20190352433
    Abstract: A process for the continuous synthesis of a modified diene elastomer comprising at least one silicon atom directly connected to the elastomer chain is provided. The process comprises polymerization by n reactors r1 to rn, considered to be continuous stirred-tank reactors equipped with an internal stirring system and arranged in series, n varying from 2 to 15. The reactor r1 is fed by an input solution comprising a solvent, one or more monomer(s), an anionic polymerization initiator chosen from lithium amides and a polar agent. The temperature of each reactor varies from 20° C. to 150° C. and is greater than or equal to the temperature of the reactor which immediately precedes it. The living diene elastomer obtained exhibits a polydispersity index varying from 1.1 to 1.7. The process further comprises modification of the living diene elastomer obtained in the preceding stage by a functionalization, coupling or star-branching agent.
    Type: Application
    Filed: December 20, 2017
    Publication date: November 21, 2019
    Applicant: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Marie-Hélène DESSENDIER, Charlotte DIRE, Claire FAUVARQUE-NUYTTEN
  • Publication number: 20180194866
    Abstract: A modified diene elastomer is provided. The elastomer comprises: at least 70% by weight, with respect to the total weight of the modified diene elastomer, of a linear diene elastomer functionalized predominantly in the middle of the chain by an alkoxysilane group, optionally partially or completely hydrolysed to give silanol, the alkoxysilane group optionally bearing another functional group capable of interacting with a reinforcing filler, the alkoxysilane group bonded to the two branches of the diene elastomer via the silicon atom, the functionalized diene elastomer exhibiting a polydispersity index before fractionalization of less than or equal to 1.6; and more than 0 and up to 30% by weight, with respect to the total weight of the modified diene elastomer, of a star-branched diene elastomer exhibiting a polydispersity index before star-branching of less than or equal to 1.6, the Mooney viscosity of the modified diene elastomer varying from 30 to 80.
    Type: Application
    Filed: July 1, 2016
    Publication date: July 12, 2018
    Applicant: COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN
    Inventors: Marie-Hélène DESSENDIER, Charlotte DIRE, Margarita DORATO, Jean Marc MARECHAL, Florent VAULTIER