    Abstract: A radiation curable aqueous coating composition having a 85° gloss of ?60 upon drying comprising (A) 10 to 99 wt % of a polyurethane, (B) 1 to 90 wt % of a radiation curable component; (C) 0.1 to 10 wt % of an associative thickener; wherein at least 80 wt % of (A)+(B)+(C) has a particle size greater than 500 nm and wherein the C?C bond concentration of the composition is 0.2 to 5.0 mmol per g of (A)+(B)+(C).
    Type: Grant
    Filed: December 23, 2013
    Date of Patent: April 25, 2017
    Assignee: DSM IP ASSETS B.V.
    Inventors: Ilse Van Casteren, Roland Tennebroek, Mario Cornelis Schoondermark, Paul De Kok
  • Publication number: 20140114010
    Abstract: A radiation curable aqueous coating composition having a 85° gloss of ?60 upon drying comprising (A) 10 to 99 wt % of a polyurethane, (B) 1 to 90 wt % of a radiation curable component; (C) 0.1 to 10 wt % of an associative thickener; wherein at least 80 wt % of (A)+(B)+(C) has a particle size greater than 500 nm and wherein the C?C bond concentration of the composition is 0.2 to 5.0 mmol per g of (A)+(B)+(C).
    Type: Application
    Filed: December 23, 2013
    Publication date: April 24, 2014
    Applicant: DSM IP ASSETS B.V.
    Inventors: Ilse VAN CASTEREN, Roland TENNEBROEK, Mario Cornelis SCHOONDERMARK, Paul DE KOK
  • Publication number: 20130184396
    Abstract: A radiation curable aqueous coating composition having a 85° gloss of ?60 upon drying comprising (A) 10 to 99 wt % of a polyurethane, (B) 1 to 90 wt % of a radiation curable component; (C) 0.1 to 10 wt % of an associative thickener; wherein at least 80 wt % of (A)+(B)+(C) has a particle size greater than 500 nm and wherein the C?C bond concentration of the composition is 0.2 to 5.0 mmol per g of (A)+(B)+(C).
    Type: Application
    Filed: March 7, 2013
    Publication date: July 18, 2013
    Applicant: DSM IP ASSETS B.V.
    Inventors: Ilse VAN CASTEREN, Roland TENNEBROEK, Mario Cornelis SCHOONDERMARK, Paul DE KOK
  • Publication number: 20120270990
    Abstract: A radiation curable aqueous coating composition having a 85° gloss of ?60 upon drying comprising (A) 10 to 99 wt % of a polyurethane, (B) 1 to 90 wt % of a radiation curable component; (C) 0.1 to 10 wt % of an associative thickener; wherein at least 80 wt % of (A)+(B)+(C) has a particle size greater than 500 nm and wherein the C?C bond concentration of the composition is 0.2 to 5.0 mmol per g of (A)+(B)+(C).
    Type: Application
    Filed: July 3, 2012
    Publication date: October 25, 2012
    Applicant: DSM IP Assets B.V.
    Inventors: Ilse VAN CASTEREN, Roland Tennebroek, Mario Cornelis Schoondermark, Paul De Kok
  • Publication number: 20100144915
    Abstract: A radiation curable aqueous coating composition having a 85° gloss of ?60 upon drying comprising (A) 10 to 99 wt % of a polyurethane, (B) 1 to 90 wt % of a radiation curable component; (C) 0.1 to 10 wt % of an associative thickener; wherein at least 80 wt % of (A)+(B)+(C) has a particle size greater than 500 nm and wherein the C?C bond concentration of the composition is 0.2 to 5.0 mmol per g of (A)+(B)+(C).
    Type: Application
    Filed: February 19, 2008
    Publication date: June 10, 2010
    Inventors: Ilse Van Casteren, Roland Tennebroek, Mario Cornelis Schoondermark, Paul De Kok