  • Patent number: 8980475
    Abstract: Process for preparing lithium mixed metal oxides which comprise essentially lithium, manganese, cobalt and nickel as metal atoms and have a stoichiometric ratio of lithium to the total transition metals of greater than 1, which comprises a) the preparation of a mixture designated as intermediate (B) which comprises essentially lithium-comprising mixed metal hydroxides and lithium-comprising mixed metal oxide hydroxides, where manganese, cobalt and nickel are comprised in the ratio (1-a-b):a:b and the oxidation state averaged over all ions of manganese, cobalt and nickel is at least 4-1.75a-1.75b, where 0?a?0.5 and 0.1?b?0.8, by a thermal treatment carried out with continual mixing and in the presence of oxygen of a mixture (A) comprising at least one transition metal compound and at least one lithium salt (L), during which L does not melt, and b) the thermal treatment carried out without mixing and in the presence of oxygen of the intermediate (B).
    Type: Grant
    Filed: June 23, 2011
    Date of Patent: March 17, 2015
    Assignee: BASF SE
    Inventors: Simon Schroedle, Hartmut Hibst, Jordan Keith Lampert, Mark Schweter, Ivan Petrovic
  • Publication number: 20110315938
    Abstract: Process for preparing lithium mixed metal oxides which comprise essentially lithium, manganese, cobalt and nickel as metal atoms and have a stoichiometric ratio of lithium to the total transition metals of greater than 1, which comprises a) the preparation of a mixture designated as intermediate (B) which comprises essentially lithium-comprising mixed metal hydroxides and lithium-comprising mixed metal oxide hydroxides, where manganese, cobalt and nickel are comprised in the ratio (1?a?b):a:b and the oxidation state averaged over all ions of manganese, cobalt and nickel is at least 4-1.75a-1.75b, where 0?a?0.5 and 0.1?b?0.8, by a thermal treatment carried out with continual mixing and in the presence of oxygen of a mixture (A) comprising at least one transition metal compound and at least one lithium salt (L), during which L does not melt, and b) the thermal treatment carried out without mixing and in the presence of oxygen of the intermediate (B).
    Type: Application
    Filed: June 23, 2011
    Publication date: December 29, 2011
    Applicant: BASF SE
    Inventors: Simon SCHROEDLE, Hartmut Hibst, Jordan Keith Lampert, Mark Schweter, Ivan Petrovic