  • Patent number: 7081172
    Abstract: A nodular graphite cast iron is provided, having a pearlite matrix, with high strength and high toughness. The nodular graphite cast iron consists essentially of, by weight %: from 3.0 to 4.6% of carbon; from 1.6 to 2.5% of silicon; from 0.2 to 0.6% of manganese; from 0.02 to 0.05% of magnesium; from 0.0004 to 0.090% of zirconium; at least one of tin and copper such that ? ranges from 0.01 to 0.06% where ? indicates a tin conversion amount defined by a summation of a weight % of the tin and 0.1× a weight % of the copper; and the balance of iron and inevitable foreign matters.
    Type: Grant
    Filed: October 14, 2003
    Date of Patent: July 25, 2006
    Assignee: Aisin Seiki Kabushiki Kaisha
    Inventors: Yasuhiro Enya, Francois Coderre, Yoshikazu Ibayashi, Masaru Matukura
  • Publication number: 20040079450
    Abstract: A nodular graphite cast iron is provided, having a pearlite matrix, with high strength and high toughness. The nodular graphite cast iron consists essentially of, by weight %: from 3.0 to 4.6% of carbon; from 1.6 to 2.5% of silicon; from 0.2 to 0.6% of manganese; from 0.02 to 0.05% of magnesium; from 0.0004 to 0.090% of zirconium; at least one of tin and copper such that &agr; ranges from 0.01 to 0.06% where a indicates a tin conversion amount defined by a summation of a weight % of the tin and 0.1× a weight % of the copper; and the balance of iron and inevitable foreign matters.
    Type: Application
    Filed: October 14, 2003
    Publication date: April 29, 2004
    Applicant: AISIN SEIKI KABUSHIKI KAISHA
    Inventors: Yasuhiro Enya, Francois Coderre, Yoshikazu Ibayashi, Masaru Matukura
  • Publication number: 20030051776
    Abstract: A nodular graphite cast iron is provided, having a pearlite matrix, with high strength and high toughness. The nodular graphite cast iron consists essentially of, by weight %,: from 3.0 to 4.6% of carbon; from 1.6 to 2.5% of silicon; from 0.2 to 0.6% of manganese; from 0.02 to 0.05% of magnesium; from 0.0004 to 0.090% of zirconium; at least one of tin and copper such that &agr; ranges from 0.01 to 0.06% where &agr; indicates a tin conversion amount defined by a summation of a weight % of the tin and 0.1×a weight % of the copper; and the balance of iron and inevitable foreign matters.
    Type: Application
    Filed: March 13, 2002
    Publication date: March 20, 2003
    Applicant: AISIN SEIKI KABUSHIKI KAISHA