  • Patent number: 10259966
    Abstract: A resin dispersion having, dispersed in water with a 50% particle diamter of at most 0.5 ?m, a polymer (C) having a hydrophilic polymer (B) or an acidic group bonded to a propylene/?-olefin copolymer (A) as a copolymer of propylene with an ?-olefin other than propylene, where the copolymer (A) has a propylene content of at least 50 mol% and less than 100 mol% and the copolymer (A) has a weight average molecular weight Mw of at least 10,000 and a molecular weight distribution Mw/Mn of at most 3.5, and the resin dispersion has a surfactant content of at most 15 parts by weight per 100 parts by weight of the polymer (C).
    Type: Grant
    Filed: October 13, 2014
    Date of Patent: April 16, 2019
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Masato Onoe, Toshiya Seko
  • Publication number: 20150125688
    Abstract: To provide an aqueous dispersion of a resin wherein dispersed particles are stable with fine particle sizes and whereby bleeding out is suppressed, which is thus useful as e.g. a surface treating agent, an adhesive or a coating material for a polyolefin substrate. A resin dispersion having, dispersed in water with a 50% particle diameter of at most 0.5 ?m, a polymer (C) having a hydrophilic polymer (B) or an acidic group bonded to a propylene/?-olefin copolymer (A) as a copolymer of propylene with an ?-olefin other than propylene, wherein the copolymer (A) has a propylene content of at least 50 mol % and less than 100 mol %, and the copolymer (A) has a weight average molecular weight Mw of at least 10,000 and a molecular weight distribution Mw/Mn of at most 3.5; and the resin dispersion has a surfactant content of at most 15 parts by weight per 100 parts by weight of the polymer (C); and a coating material or laminate, made by using such a dispersion.
    Type: Application
    Filed: October 13, 2014
    Publication date: May 7, 2015
    Applicant: Mitsubishi Chemical Corporation
    Inventors: Masato ONOE, Toshiya Seko
  • Publication number: 20120135243
    Abstract: To provide an aqueous dispersion of a resin wherein dispersed particles are stable with fine particle sizes and whereby bleeding out is suppressed, which is thus useful as e.g. a surface treating agent for a polyolefin substrate, an adhesive or a coating material. A resin dispersion having dispersed in water a polymer (C) having a hydrophilic polymer (B) bonded to a polyolefin (A) in a ratio of (A):(B)=100:5 to 100:500 (weight ratio); a method for producing the resin dispersion; and a coating material and a laminate, employing it.
    Type: Application
    Filed: February 3, 2012
    Publication date: May 31, 2012
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Masato ONOE, Toshiya Seko, Yongwoo Shin, Yongjun Jang, Fumihiko Shimizu
  • Patent number: 8158727
    Abstract: To provide an aqueous dispersion of a resin wherein dispersed particles are stable with fine particle sizes and whereby bleeding out is suppressed, which is thus useful as e.g. a surface treating agent for a polyolefin substrate, an adhesive or a coating material. A resin dispersion having dispersed in water a polymer (C) having a hydrophilic polymer (B) bonded to a polyolefin (A) in a ratio of (A):(B)=100:5 to 100:500 (weight ratio); a method for producing the resin dispersion; and a coating material and a laminate, employing it.
    Type: Grant
    Filed: June 2, 2006
    Date of Patent: April 17, 2012
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Masato Onoe, Toshiya Seko, Yongwoo Shin, Yongjun Jang, Fumihiko Shimizu
  • Patent number: 7659356
    Abstract: A polypropylene type aqueous dispersion comprising the following components (a) to (c): (a) a polypropylene type polymer 100 parts by weight and/or a modified polypropylene type polymer (b) a surfactant 1 to 100 parts by weight, and (c) water 100 to 1,000 parts by weight, wherein the component (a) has a main chain having the following features (1) and (2) and dispersion particles in the dispersion have an average particle size of at most 0.5 ?m, Feature (1) when observing a peak derived from a carbon atom of a methyl group in a propylene unit chain part comprising a head-to-tail bond by 13C-NMR and fixing a chemical shift of a peak top at a peak attributable to pentad expressed by mmmm to 21.8 ppm, a ratio (S1/S) of an area S1 of a peak of a peak top at 21.8 ppm to a total area S of peaks at from 19.8 ppm to 22.1 ppm is at least 10% and at most 60%, and when an area of a peak (mmmr) of a peak top at 21.5 to 21.
    Type: Grant
    Filed: August 4, 2008
    Date of Patent: February 9, 2010
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Teruaki Ashihara, Masato Onoe, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Yukihito Zanka, Kouichi Nakayama
  • Publication number: 20090226728
    Abstract: To provide an aqueous dispersion of a resin wherein dispersed particles are stable with fine particle sizes and whereby bleeding out is suppressed, which is thus useful as e.g. a surface treating agent for a polyolefin substrate, an adhesive or a coating material. A resin dispersion having dispersed in water a polymer (C) having a hydrophilic polymer (B) bonded to a polyolefin (A) in a ratio of (A):(B)=100:5 to 100:500 (weight ratio); a method for producing the resin dispersion; and a coating material and a laminate, employing it.
    Type: Application
    Filed: June 2, 2006
    Publication date: September 10, 2009
    Inventors: Masato Onoe, Toshiya Seko, Yongwoo Shin, Yongjun Jang, Fumihiko Shimizu
  • Publication number: 20090092847
    Abstract: To provide an aqueous dispersion of a resin wherein dispersed particles are stable with fine particle sizes and whereby bleeding out is suppressed, which is thus useful as e.g. a surface treating agent, an adhesive or a coating material for a polyolefin substrate. A resin dispersion having, dispersed in water with a 50% particle diameter of at most 0.5 ?m, a polymer (C) having a hydrophilic polymer (B) or an acidic group bonded to a propylene/?-olefin copolymer (A) as a copolymer of propylene with an ?-olefin other than propylene, wherein the copolymer (A) has a propylene content of at least 50 mol % and less than 100 mol %, and the copolymer (A) has a weight average molecular weight Mw of at least 10,000 and a molecular weight distribution Mw/Mn of at most 3.5; and the resin dispersion has a surfactant content of at most 15 parts by weight per 100 parts by weight of the polymer (C); and a coating material or laminate, made by using such a dispersion.
    Type: Application
    Filed: December 1, 2006
    Publication date: April 9, 2009
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Masato Onoe, Toshiya Seko
  • Publication number: 20090018251
    Abstract: A polypropylene type aqueous dispersion comprising the following components (a) to (c): (a) a polypropylene type polymer 100 parts by weight and/or a modified polypropylene type polymer (b) a surfactant 1 to 100 parts by weight, and (c) water 100 to 1,000 parts by weight, wherein the component (a) has a main chain having the following features (1) and (2) and dispersion particles in the dispersion have an average particle size of at most 0.5 ?m, Feature (1) when observing a peak derived from a carbon atom of a methyl group in a propylene unit chain part comprising a head-to-tail bond by 13C-NMR and fixing a chemical shift of a peak top at a peak attributable to pentad expressed by mmmm to 21.8 ppm, a ratio (S1/S) of an area S1 of a peak of a peak top at 21.8 ppm to a total area S of peaks at from 19.8 ppm to 22.1 ppm is at least 10% and at most 60%, and when an area of a peak (mmmr) of a peak top at 21.5 to 21.
    Type: Application
    Filed: August 4, 2008
    Publication date: January 15, 2009
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Teruaki ASHIHARA, Masato ONOE, Kazuyuki HATA, Fumihiko SHIMIZU, Naomasa SATO, Yukihito ZANKA, Kouichi NAKAYAMA
  • Patent number: 7304111
    Abstract: A problem of the invention is to provide a propylene copolymer which is excellent in adhesion to crystalline propylene-based polymers and which is excellent in solubility and compatibility with polar resins, a process for producing the same, and a composition containing the subject polypropylene copolymer. The invention is concerned with a polypropylene copolymer, which is characterized by having a polymer principal chain (A) derived from a propylene-based polymer having (1) a prescribed requirement as defined by the 13C-NMR spectral measurement and having (2) a melting point [Tm] by a differential scanning calorimeter of not higher than 100° C., or a crystal melting heat of less than 5 J/g; and a side chain containing a polymer chain (B) which is different from the principal chain, with a weight ratio of (A)/(B) being in the range of from 20/1 to 1/20, a composition containing the subject copolymer, and a process for producing the subject copolymer.
    Type: Grant
    Filed: August 22, 2005
    Date of Patent: December 4, 2007
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Masato Onoe, Kazuyuki Hata
  • Publication number: 20070166250
    Abstract: The present invention discloses a cosmetic polymer composition containing a straight-chain block copolymer, where the copolymer having a unit derived from a compound having an ethylenic unsaturated bond, having a number-average molecular weight of 1.0×103 to 1.0×106, and having at least two or more glass transition points or melting points; a hair cosmetic polymer composition containing a copolymer a copolymer capable of forming a film having a Young's modulus of 50 MPa or larger and a fracture-point elongation of 100% or larger, and dispersible into water and/or alcohol; and a cosmetic material containing these compositions.
    Type: Application
    Filed: March 29, 2007
    Publication date: July 19, 2007
    Inventors: Tomoaki HIWATASHI, Minako SHIBATA, Osamu NISHIZAWA, Masato ONOE, Yasuo KITANI
  • Patent number: 7122604
    Abstract: This invention provides a graft modified polypropylene polymer which does not contain halogens, is excellent in certain properties such as solubility and can add good adhesiveness and coating ability to crystalline propylene polymer base materials, and a composition containing the same; and in particular, it provides a propylene polymer which contains a propylene polymer main chain having a stereo-block structure containing an isotactic block and a side chain containing a carboxylic acid group, an acid anhydride group or a carboxylic acid ester group, wherein when it is dissolved in toluene to a concentration of 10% by weight at 25° C., the insoluble matter is 1% by weight or less based on the total polymer, and a composition containing the same.
    Type: Grant
    Filed: November 12, 2004
    Date of Patent: October 17, 2006
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Masato Onoe, Teruaki Ashihara, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Akio Tanna
  • Publication number: 20060025535
    Abstract: A problem of the invention is to provide a propylene copolymer which is excellent in adhesion to crystalline propylene-based polymers and which is excellent in solubility and compatibility with polar resins, a process for producing the same, and a composition containing the subject polypropylene copolymer. The invention is concerned with a polypropylene copolymer, which is characterized by having a polymer principal chain (A) derived from a propylene-based polymer having (1) a prescribed requirement as defined by the 13C-NMR spectral measurement and having (2) a melting point [Tm] by a differential scanning calorimeter of not higher than 100° C., or a crystal melting heat of less than 5 J/g; and a side chain containing a polymer chain (B) which is different from the principal chain, with a weight ratio of (A)/(B) being in the range of from 20/1 to 1/20, a composition containing the subject copolymer, and a process for producing the subject copolymer.
    Type: Application
    Filed: August 22, 2005
    Publication date: February 2, 2006
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Masato Onoe, Kazuyuki Hata
  • Publication number: 20050124753
    Abstract: A polypropylene type aqueous dispersion comprising the following components (a) to (c): (a) a polypropylene type polymer 100 parts by weight and/or a modified polypropylene type polymer (b) a surfactant 1 to 100 parts by weight, and (c) water 100 to 1,000 parts by weight, wherein the component (a) has a main chain having the following features (1) and (2) and dispersion particles in the dispersion have an average particle size of at most 0.5 ?m, Feature (1) when observing a peak derived from a carbon atom of a methyl group in a propylene unit chain part comprising a head-to-tail bond by 13C-NMR and fixing a chemical shift of a peak top at a peak attributable to pentad expressed by mmmm to 21.8 ppm, a ratio (S1/S) of an area S1 of a peak of a peak top at 21.8 ppm to a total area S of peaks at from 19.8 ppm to 22.1 ppm is at least 10% and at most 60%, and when an area of a peak (mmmr) of a peak top at 21.5 to 21.
    Type: Application
    Filed: October 26, 2004
    Publication date: June 9, 2005
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Teruaki Ashihara, Masato Onoe, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Yukihito Zanka, Kouichi Nakayama
  • Patent number: 6887943
    Abstract: This invention provides a graft modified polypropylene polymer which does not contain halogens, is excellent in certain properties such as solubility and can add good adhesiveness and coating ability to crystalline propylene polymer base materials, and a composition containing the same; and in particular, it provides a propylene polymer which contains a propylene polymer main chain having a stereo-block structure containing an isotactic block and a side chain containing a carboxylic acid group, an acid anhydride group or a carboxylic acid ester group, wherein when it is dissolved in toluene to a concentration of 10% by weight at 25° C., the insoluble matter is 1% by weight or less based on the total polymer, and a composition containing the same.
    Type: Grant
    Filed: October 31, 2002
    Date of Patent: May 3, 2005
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Masato Onoe, Teruaki Ashihara, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Akio Tanna
  • Publication number: 20050075441
    Abstract: This invention provides a graft modified polypropylene polymer which does not contain halogens, is excellent in certain properties such as solubility and can add good adhesiveness and coating ability to crystalline propylene polymer base materials, and a composition containing the same; and in particular, it provides a propylene polymer which contains a propylene polymer main chain having a stereo-block structure containing an isotactic block and a side chain containing a carboxylic acid group, an acid anhydride group or a carboxylic acid ester group, wherein when it is dissolved in toluene to a concentration of 10% by weight at 25° C., the insoluble matter is 1% by weight or less based on the total polymer, and a composition containing the same.
    Type: Application
    Filed: November 12, 2004
    Publication date: April 7, 2005
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Masato Onoe, Teruaki Ashihara, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Akio Tanna
  • Publication number: 20040223933
    Abstract: The present invention discloses a cosmetic polymer composition containing a straight-chain block copolymer, where the copolymer having a unit derived from a compound having an ethylenic unsaturated bond, having a number-average molecular weight of 1.0×103 to 1.0×106, and having at least two or more glass transition points or melting points; a hair cosmetic polymer composition containing a copolymer a copolymer capable of forming a film having a Young's modulus of 50 MPa or larger and a fracture-point elongation of 100% or larger, and dispersible into water and/or alcohol; and a cosmetic material containing these compositions.
    Type: Application
    Filed: March 12, 2004
    Publication date: November 11, 2004
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Tomoaki Hiwatashi, Minako Shibata, Osamu Nishizawa, Masato Onoe, Yasuo Kitani
  • Publication number: 20030153686
    Abstract: This invention provides a graft modified polypropylene polymer which does not contain halogens, is excellent in certain properties such as solubility and can add good adhesiveness and coating ability to crystalline propylene polymer base materials, and a composition containing the same; and in particular, it provides a propylene polymer which contains a propylene polymer main chain having a stereo-block structure containing an isotactic block and a side chain containing a carboxylic acid group, an acid anhydride group or a carboxylic acid ester group, wherein when it is dissolved in toluene to a concentration of 10% by weight at 25° C., the insoluble matter is 1% by weight or less based on the total polymer, and a composition containing the same.
    Type: Application
    Filed: October 31, 2002
    Publication date: August 14, 2003
    Applicant: MITSUBISHI CHEMICAL CORPORATION
    Inventors: Masato Onoe, Teruaki Ashihara, Kazuyuki Hata, Fumihiko Shimizu, Naomasa Sato, Akio Tanna
  • Patent number: 6100347
    Abstract: A crystalline olefin base resin composition having a high elastic modulus, a high heat resistance and excellent scratch resistance, and that is useful as a material for car parts and the like is provided. The crystalline olefin base resin composition described above comprises 99 to 40% by weight of the following component (A) and 1 to 60% by weight of the following component (B):(A) a crystalline olefin base resin, and(B) a polymer obtained by vinylene polymerization of cyclic olefin and having a weight-average molecular weight of not less than 1,000 and less than 10,000 and a glass transition point of from 140 to 400.degree. C.
    Type: Grant
    Filed: April 23, 1998
    Date of Patent: August 8, 2000
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Yuuta Kumano, Osamu Nisizawa, Kenji Takasaki, Masato Onoe