  • Patent number: 10132007
    Abstract: The present invention provides a fabricating method for meltblown nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps. Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, prepare blending mucilage from mixing cellulose serum via blending process. Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fifthly, produce molten filament tow by meltblown spinning method in association with coagulation, regeneration in coagulation bath, and water rinse.
    Type: Grant
    Filed: November 10, 2015
    Date of Patent: November 20, 2018
    Assignee: ACELON CHEMICALS AND FIBER CORPORATION
    Inventors: Wen-Tung Chou, Ming-Yi Lai, Kun-Shan Huang, Shao-Hua Chou, Meng-Heng Hsieh
  • Patent number: 10132009
    Abstract: The present invention provides a fabricating method for natural cellulose fiber blended with nano silver. The fabricating method comprises following steps: Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fourthly, produce fibrous tow by Dry-Jet Wet Spinning method in association with coagulation, regeneration in coagulation bath, and water rinse. Finally, obtain final product of natural cellulose fiber blended with nano silver by post treatments of dry, oil and coil in proper order.
    Type: Grant
    Filed: November 9, 2015
    Date of Patent: November 20, 2018
    Assignee: ACELON CHEMICALS AND FIBER CORPORATION
    Inventors: Wen-Tung Chou, Ming-Yi Lai, Kun-Shan Huang, Shao-Hua Chou, Meng-Heng Hsieh
  • Patent number: 10094049
    Abstract: The present invention provides a fabricating method for spunbond nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps. Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, prepare blending mucilage from mixing cellulose serum via blending process. Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fifthly, produce molten filament tow by spunbond spinning method in association with coagulation, regeneration, water rinse and high-speed stretching process.
    Type: Grant
    Filed: November 12, 2015
    Date of Patent: October 9, 2018
    Assignee: ACELON CHEMICALS AND FIBER CORPORATION
    Inventors: Wen-Tung Chou, Ming-Yi Lai, Kun-Shan Huang, Shao-Hua Chou, Meng-Heng Hsieh
  • Publication number: 20160333498
    Abstract: The present invention provides a fabricating method for natural cellulose fiber blended with nano silver. The fabricating method comprises following steps: Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fourthly, produce fibrous tow by Dry-Jet Wet Spinning method in association with coagulation, regeneration in coagulation bath, and water rinse. Finally, obtain final product of natural cellulose fiber blended with nano silver by post treatments of dry, oil and coil in proper order.
    Type: Application
    Filed: November 9, 2015
    Publication date: November 17, 2016
    Inventors: Wen-Tung CHOU, Ming-Yi LAI, Kun-Shan HUANG, Shao-Hua CHOU, Meng-Heng HSIEH
  • Publication number: 20160333499
    Abstract: The present invention provides a fabricating method for meltblown nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps. Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, prepare blending mucilage from mixing cellulose serum via blending process. Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fifthly, produce molten filament tow by meltblown spinning method in association with coagulation, regeneration in coagulation bath, and water rinse.
    Type: Application
    Filed: November 10, 2015
    Publication date: November 17, 2016
    Inventors: Wen-Tung CHOU, Ming-Yi LAI, Kun-Shan HUANG, Shao-Hua CHOU, Meng-Heng HSIEH
  • Publication number: 20160333508
    Abstract: The present invention provides a fabricating method for spunbond nonwoven from natural cellulose fiber blended with nano silver, which comprises following steps. Firstly, prepare nano silver colloidal sol by reduction titration for mixture of polyvinyl alcohol (PVA), silver nitrate (AgNO3) and sodium borohydride (NaBH4). Secondly, prepare mixing cellulose serum by blending agitation for mixture of wood pulp, N-methylmorpholine N-oxide (NMMO) and stabilizer. Thirdly, prepare blending mucilage from mixing cellulose serum via blending process. Fourthly, produce spinning dope by blending and dehydrating the nano silver colloidal sol and mixing cellulose serum. Fifthly, produce molten filament tow by spunbond spinning method in association with coagulation, regeneration, water rinse and high-speed stretching process.
    Type: Application
    Filed: November 12, 2015
    Publication date: November 17, 2016
    Inventors: Wen-Tung CHOU, Ming-Yi LAI, Kun-Shan HUANG, Shao-Hua CHOU, Meng-Heng HSIEH